Arkema Group Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyether block amide PEBAX® MV 1074 SA 01 MED is a thermoplastic elastomer made of hydrophilic flexible polyether and rigid polyamide. PEBAX® MV 1074 SA 01 MED is an inherently dissipative polymer and can be dry blended or compounded with an isolative polymer to lower the surface resistivity. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applications such as minimally invasive devices.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Water Absorption 48 %
48 %
24 hr in water at 20°C; ISO 62
Moisture Absorption at Equilibrium 1.4 %
1.4 %
50% RH; ISO 62
Water Absorption at Saturation 0.50 %
0.50 %
20°C and 65% RH; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
50% RH; ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
50% RH; ASTM D638
Elongation at Break >= 700 %
>= 700 %
50% RH; ASTM D638
Flexural Modulus 0.0800 GPa
11.6 ksi
50% RH; ISO 178
Thermal Properties Metric English Comments
Melting Point 158 °C
316 °F
ISO 11357
Optical Properties Metric English Comments
Refractive Index 1.502
1.502
Electrical Properties Metric English Comments
Volume Resistivity 2.5e+9 ohm-cm
2.5e+9 ohm-cm
50% RH; IEC 60093
Surface Resistance 3e+9 ohm

@Temperature 20.0 °C
3e+9 ohm

@Temperature 68.0 °F
50% RH; IEC 60093
Static Decay <= 1 sec
<= 1 sec
MIL B-81705