Noltex Soarnol® H4815 Ethylene Vinyl Alcohol Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Alcohol (EVOH)
Manufacturer Noltex
Trade Name Soarnol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Noltex Soarnol® H4815 Ethylene Vinyl Alcohol Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Special designed the highest ethylene content grade. Ethylene content 48 mol%.Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon Gohsei.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 210 °C
16 g/10 min

@Load 4.76 lb,
Temperature 410 °F
Thermal Properties Metric English Comments
Melting Point 158 °C
316 °F
Optical Properties Metric English Comments
Refractive Index 1.513
1.513
Quenched
1.524
1.524
Annealed at 140°C, 30 min