ExxonMobil Escorene™ UL 00728 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 00728 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 00728 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoFree Flowing Agent: No Applications: CompoundingInjection MoldingExtrudable AdhesivesWire and Cable Compounds Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ExxonMobil method
Vinyl Acetate Content 27.5 %
27.5 %
ExxonMobil method
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.689 MPa
100 psi
Molded Properties; ISO 527-2/1A/100
Tensile Modulus 0.0159 GPa
2.30 ksi
Molded Properties; ISO 527-2/1
Thermal Properties Metric English Comments
Melting Point <= 158 °C
<= 316 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 42.8 °C
109 °F
ASTM D1525
Descriptive Properties Value Comments
Blending Temperature 220
Users viewing this material also viewed the following: