Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solef® 5130 PVDF has an ultra high viscosity ideal for its usage in lithium batteries.Additional Information: Intrinsic Viscosity: 0.27 - 0.37 l/gInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.75 - 1.78 g/cc
0.0632 - 0.0643 lb/in³
ISO 1183
Water Absorption <= 0.20 %

@Temperature 23.0 °C,
Time 86400 sec
<= 0.20 %

@Temperature 73.4 °F,
Time 24.0 hour
30g; ASTM D543
Mechanical Properties Metric English Comments
Tensile Modulus 1.00 - 1.50 GPa

@Temperature 23.0 °C
145 - 218 ksi

@Temperature 73.4 °F
1.0 mm/min; ASTM D638
Thermal Properties Metric English Comments
Heat of Fusion 40.0 - 48.0 J/g
17.2 - 20.6 BTU/lb
80°C to end of melting; ASTM D3418
Melting Point 158 - 166 °C
316 - 331 °F
ASTM D3418
Crystallization Temperature 135 - 140 °C
275 - 284 °F
Peak, DSC; ASTM D3418
Glass Transition Temp, Tg -40.0 °C
-40.0 °F
DSC
Decomposition Temperature >= 375 °C
>= 707 °F
@ 1% weight loss; TGA
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Intensity = 10 mA, after 2 min @ 23°C; ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
Voltage < 1V, after 2 min - 500 V @ 23°C; ASTM D257
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Very high Viscosity
Generic PVDF
Uses Batteries
Binder