ExxonMobil Escorene™ FL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ FL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: FL 00728CC is an excellent coextrusion partner in extrusion coating, blown and cast film. Good adhesion onto OPP in coextrusion. This grade offers excellent optical, low gel and a very low Seal Initiation Temperature in sealing applications. Processing Conditions: Excellent results are obtained in extrusion coating at 200°C (392°F) temperature range. Processing temperatures above 220°C (428°F) may cause resin degradation. FL 00728CC should be fed into the extruder after LDPE of a similar or higher melt index. Machines should always be purged with LDPE or a suitable cleaning compound before shutdown.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications:Adhesive LaminationAdhesive Layer onto OPPCling LayerCoextrusion CoatingCompoundingExtrusion CoatingExtrusion LaminationHigh Frequency Sealing Industrial PackagingInjection MoldingMasterbatch Base ResinSurface Protection FilmThermal LaminationInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ExxonMobil method
Vinyl Acetate Content 27.5 %
27.5 %
ExxonMobil method
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 80

@Time 15.0 sec
80

@Time 0.00417 hour
Molded Properties; ISO 868
Tensile Strength at Break >= 0.689 MPa
>= 100 psi
Molded Properties; ISO 527-2/1A/100
Tensile Modulus 0.0159 GPa
2.30 ksi
Molded Properties; ISO 527-2/1
Thermal Properties Metric English Comments
Melting Point <= 158 °C
<= 316 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 42.8 °C
109 °F
ASTM D1525
Descriptive Properties Value Comments
Blending Temperature 220