Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 CV20 Nylon 6.6 for injection molding, 20% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.60 - 5.50 J/cm² | 12.4 - 26.2 ft-lb/in² | Average value: 3.77 J/cm² Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.60 - 7.20 J/cm² | 12.4 - 34.3 ft-lb/in² | Average value: 4.53 J/cm² Grade Count:8 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Charpy Impact Unnotched | 2.60 - 6.50 J/cm² | 12.4 - 30.9 ft-lb/in² | Average value: 4.16 J/cm² Grade Count:20 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-8114 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 2205-7123 Blend based on polyaryl ether ketone, with carbon fiber, PTFE, lubricant modified Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr.. |
|||
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® CMH454 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® MH254 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-7731/BL PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |
|||
Charpy Impact Unnotched | 2.60 J/cm² @Temperature -30.0 °C |
12.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | IS0179 |
Zhejiang Juner 302-G10 10% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | ISO 179 |
BASF Ultradur B 4040 G4 LS High Speed BK15029 20% Glass Filled PBT/PET |
|||
Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | ISO 179/1eU |
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, .. |
|||
Charpy Impact Unnotched | 2.60 - 3.50 J/cm² | 12.4 - 16.7 ft-lb/in² | Average value: 3.03 J/cm² Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |