Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 CV20 Nylon 6.6 for injection molding, 20% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.60 - 5.50 J/cm²
12.4 - 26.2 ft-lb/in²
Average value: 3.77 J/cm² Grade Count:3
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.60 - 7.20 J/cm²
12.4 - 34.3 ft-lb/in²
Average value: 4.53 J/cm² Grade Count:8
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Charpy Impact Unnotched 2.60 - 6.50 J/cm²
12.4 - 30.9 ft-lb/in²
Average value: 4.16 J/cm² Grade Count:20
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 20-8114 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 2205-7123 Blend based on polyaryl ether ketone, with carbon fiber, PTFE, lubricant modified
Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr..
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® CMH454 Acrylic Polymer
Information provided by Lucite International
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® MH254 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1105-7731/BL PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
Charpy Impact Unnotched 2.60 J/cm²

@Temperature -30.0 °C
12.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
IS0179
Zhejiang Juner 302-G10 10% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
ISO 179
BASF Ultradur B 4040 G4 LS High Speed BK15029 20% Glass Filled PBT/PET
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
ISO 179/1eU
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET
Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, ..
Charpy Impact Unnotched 2.60 - 3.50 J/cm²
12.4 - 16.7 ft-lb/in²
Average value: 3.03 J/cm² Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..