Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 2.00 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.230 - 2.00 J/cm²
1.09 - 9.52 ft-lb/in²
Average value: 0.820 J/cm² Grade Count:50
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Charpy Impact, Notched 0.170 - 2.00 J/cm²
0.809 - 9.52 ft-lb/in²
Average value: 0.756 J/cm² Grade Count:123
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Charpy Impact, Notched 0.100 - 2.00 J/cm²
0.476 - 9.52 ft-lb/in²
Average value: 1.00 J/cm² Grade Count:4
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Charpy Impact, Notched 0.550 - 2.00 J/cm²

@Temperature -30.0 - -30.0 °C
2.62 - 9.52 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.974 J/cm² Grade Count:34
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Charpy Impact, Notched 0.140 - 2.00 J/cm²
0.666 - 9.52 ft-lb/in²
Average value: 0.508 J/cm² Grade Count:38
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Charpy Impact, Notched 0.610 - 2.00 J/cm²

@Temperature -30.0 - -20.0 °C
2.90 - 9.52 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 1.17 J/cm² Grade Count:30
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Charpy Impact, Notched 0.200 - 2.00 J/cm²
0.952 - 9.52 ft-lb/in²
Average value: 0.650 J/cm² Grade Count:7
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Charpy Impact, Notched 0.400 - 2.00 J/cm²
1.90 - 9.52 ft-lb/in²
Average value: 1.42 J/cm² Grade Count:24
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.600 - 2.00 J/cm²

@Temperature -30.0 - 30.0 °C
2.86 - 9.52 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.996 J/cm² Grade Count:13
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Charpy Impact, Notched 1.00 - 2.00 J/cm²

@Temperature -30.0 - 30.0 °C
4.76 - 9.52 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.52 J/cm² Grade Count:20
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Charpy Impact, Notched 0.150 - 2.00 J/cm²

@Temperature -30.0 - -20.0 °C
0.714 - 9.52 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.863 J/cm² Grade Count:43
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Charpy Impact, Notched 2.00 - 2.00 J/cm²

@Temperature -30.0 - -30.0 °C
9.52 - 9.52 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.00 J/cm² Grade Count:2
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..
Charpy Impact, Notched 0.100 - 2.00 J/cm²

@Temperature -40.0 - -20.0 °C
0.476 - 9.52 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.596 J/cm² Grade Count:39
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Charpy Impact, Notched 0.0300 - 2.00 J/cm²

@Temperature -30.0 - -20.0 °C
0.143 - 9.52 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.413 J/cm² Grade Count:58
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..