Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Acrylic, General Purpose, Molded

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylic, General Purpose, Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.700 - 1.20 g/cc
0.0253 - 0.0434 lb/in³
Average value: 1.17 g/cc Grade Count:249
Water Absorption 0.300 - 2.00 %
0.300 - 2.00 %
Average value: 0.461 % Grade Count:96
Moisture Absorption at Equilibrium 0.300 - 0.600 %
0.300 - 0.600 %
Average value: 0.399 % Grade Count:29
Water Absorption at Saturation 0.300 - 2.20 %
0.300 - 2.20 %
Average value: 1.23 % Grade Count:21
Linear Mold Shrinkage 0.00200 - 0.00800 cm/cm
0.00200 - 0.00800 in/in
Average value: 0.00455 cm/cm Grade Count:174
Melt Flow 0.112 - 40.0 g/10 min
0.112 - 40.0 g/10 min
Average value: 8.51 g/10 min Grade Count:239
Mechanical Properties Metric English Comments
Hardness, Rockwell L 40.0 - 54.0
40.0 - 54.0
Average value: 46.0 Grade Count:3
Hardness, Rockwell M 18.0 - 99.0
18.0 - 99.0
Average value: 81.9 Grade Count:99
Hardness, Rockwell R 69.0
69.0
Average value: 69.0 Grade Count:4
Ball Indentation Hardness 170 - 190 MPa
24700 - 27600 psi
Average value: 179 MPa Grade Count:21
Tensile Strength, Ultimate 19.3 - 85.0 MPa
2800 - 12300 psi
Average value: 64.0 MPa Grade Count:200
Tensile Strength, Yield 25.0 - 85.0 MPa
3630 - 12300 psi
Average value: 60.5 MPa Grade Count:51
Elongation at Break 1.00 - 85.0 %
1.00 - 85.0 %
Average value: 10.3 % Grade Count:244
Elongation at Yield 2.00 - 6.00 %
2.00 - 6.00 %
Average value: 4.54 % Grade Count:58
Modulus of Elasticity 0.950 - 3.79 GPa
138 - 550 ksi
Average value: 2.89 GPa Grade Count:192
Flexural Yield Strength 33.1 - 143 MPa
4800 - 20700 psi
Average value: 100 MPa Grade Count:198
Flexural Modulus 1.17 - 3.59 GPa
170 - 520 ksi
Average value: 2.79 GPa Grade Count:100
Compressive Yield Strength 36.5 - 117 MPa
5300 - 17000 psi
Average value: 102 MPa Grade Count:8
Izod Impact, Notched 0.118 - 1.47 J/cm
0.220 - 2.76 ft-lb/in
Average value: 0.297 J/cm Grade Count:163
0.240255 - 0.37373 J/cm

@Temperature 0.000 - 0.000 °C
0.450096 - 0.70015 ft-lb/in

@Temperature 32.0 - 32.0 °F
Average value: 0.463 J/cm Grade Count:6
0.10678 - 0.80085 J/cm

@Temperature 0.000 - 0.000 °C
0.20004 - 1.5003 ft-lb/in

@Temperature 32.0 - 32.0 °F
Average value: 0.463 J/cm Grade Count:10
0.10678 - 0.80085 J/cm

@Thickness 3.17 - 6.35 mm
0.20004 - 1.5003 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 0.463 J/cm Grade Count:10
0.26695 - 0.85424 J/cm

@Diameter 6.35 - 6.35 mm
0.50011 - 1.6003 ft-lb/in

@Diameter 0.250 - 0.250 in
Average value: 0.463 J/cm Grade Count:6
0.26695 - 0.85424 J/cm

@Temperature 0.000 - 0.000 °C
0.50011 - 1.6003 ft-lb/in

@Temperature 32.0 - 32.0 °F
Average value: 0.463 J/cm Grade Count:6
Izod Impact, Notched (ISO) 1.30 - 19.0 kJ/m²
0.619 - 9.04 ft-lb/in²
Average value: 3.13 kJ/m² Grade Count:23
Charpy Impact Unnotched 1.00 J/cm² - NB
4.76 ft-lb/in² - NB
Average value: 2.91 J/cm² Grade Count:56
Charpy Impact, Notched 0.140 - 2.00 J/cm²
0.666 - 9.52 ft-lb/in²
Average value: 0.508 J/cm² Grade Count:38
Gardner Impact 0.226 - 0.339 J
0.167 - 0.250 ft-lb
Average value: 0.231 J Grade Count:92
Falling Dart Impact 2.17 - 18.6 J
1.60 - 13.7 ft-lb
Average value: 10.7 J Grade Count:4
Tensile Creep Modulus, 1 hour 1800 - 2700 MPa
261000 - 392000 psi
Average value: 2460 MPa Grade Count:9
Tensile Creep Modulus, 1000 hours 1200 - 1800 MPa
174000 - 261000 psi
Average value: 1580 MPa Grade Count:10
Taber Abrasion, mg/1000 Cycles 16.5
16.5
Average value: 16.5 Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 30.0 - 150 µm/m-°C
16.7 - 83.3 µin/in-°F
Average value: 70.2 µm/m-°C Grade Count:168
72.0 - 149.4 µm/m-°C

@Temperature -17.8 - 156 °C
40.0 - 83.00 µin/in-°F

@Temperature 0.000 - 312 °F
Average value: 94.9 µm/m-°C Grade Count:26
Specific Heat Capacity 1.46 - 1.50 J/g-°C
0.349 - 0.359 BTU/lb-°F
Average value: 1.47 J/g-°C Grade Count:9
Thermal Conductivity 0.187 - 0.216 W/m-K
1.30 - 1.50 BTU-in/hr-ft²-°F
Average value: 0.202 W/m-K Grade Count:15
Maximum Service Temperature, Air 50.0 - 98.0 °C
122 - 208 °F
Average value: 83.9 °C Grade Count:68
Deflection Temperature at 0.46 MPa (66 psi) 73.0 - 109 °C
163 - 228 °F
Average value: 96.8 °C Grade Count:61
Deflection Temperature at 1.8 MPa (264 psi) 51.7 - 106 °C
125 - 223 °F
Average value: 89.2 °C Grade Count:211
Vicat Softening Point 58.3 - 119 °C
137 - 246 °F
Average value: 100 °C Grade Count:231
Annealing Point 60.0 - 90.0 °C
140 - 194 °F
Average value: 77.1 °C Grade Count:7
Heat Distortion Temperature 85.0 - 105 °C
185 - 221 °F
Average value: 96.4 °C Grade Count:7
Glass Transition Temp, Tg 102 - 122 °C
216 - 252 °F
Average value: 110 °C Grade Count:21
Flammability, UL94 HB
HB
Grade Count:160
Oxygen Index 18.0 %
18.0 %
Average value: 18.0 % Grade Count:7
Glow Wire Test 650 - 700 °C
1200 - 1290 °F
Average value: 662 °C Grade Count:30
Optical Properties Metric English Comments
Refractive Index 1.49 - 1.52
1.49 - 1.52
Average value: 1.49 Grade Count:106
Haze 0.400 - 98.0 %
0.400 - 98.0 %
Average value: 7.35 % Grade Count:163
Yellow Index -7.50 - 6.50 %
-7.50 - 6.50 %
Average value: 0.758 % Grade Count:25
Transmission, Visible 74.0 - 93.0 %
74.0 - 93.0 %
Average value: 90.5 % Grade Count:233
UV Transmittance 0.190 - 88.5 %
0.190 - 88.5 %
Average value: 39.8 % Grade Count:5
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+10 - 1.00e+17 ohm-cm
1.00e+10 - 1.00e+17 ohm-cm
Average value: 3.49e+15 ohm-cm Grade Count:36
Surface Resistance 2.60e+9 - 1.00e+16 ohm
2.60e+9 - 1.00e+16 ohm
Average value: 1.17e+15 ohm Grade Count:25
Dielectric Constant 2.80 - 4.00
2.80 - 4.00
Average value: 3.45 Grade Count:32
Dielectric Strength 0.787 - 60.0 kV/mm
20.0 - 1520 kV/in
Average value: 25.5 kV/mm Grade Count:39
Dissipation Factor 0.0200 - 0.190
0.0200 - 0.190
Average value: 0.0488 Grade Count:34
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:16
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved