Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.140 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.140 - 0.200 J/cm²
0.666 - 0.952 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group MELOPAS® 2010 MF Melamine
Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav..
Charpy Impact, Notched >= 0.140 J/cm²
>= 0.666 ft-lb/in²
ISO 179
Perstorp Compounds AMITEC VXO UF/MF blend
A special Urea Formaldehyde/Melamine Formaldehyde blend that enhances surface properties and is optimized for cost-effective injection molding of visible components.Information provided by Perstorp ..
Charpy Impact, Notched 0.140 - 2.00 J/cm²
0.666 - 9.52 ft-lb/in²
Average value: 0.508 J/cm² Grade Count:38
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed  (disc
Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed &nbs
Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 12404 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage  (discontinued **)&
Phenolic molding compound, inorganically/organically filled, good dimensional stability, low shrinkage.Application areas: Housing parts for gas meter.Information provided by Bak AGBak AG became a pa..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 14600 Phenolic Formaldehyde Resin, High Surface Quality  (discontinued **)
Phenolic molding compound, mainly organically filled, low specific gravity.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a part of Hexion in 2005..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 14694 Phenolic Formaldehyde Resin, High Surface Quality  (discontinued **)
Phenolic molding compound, mainly organically filled, very soft flow for large molds.Application areas: Housing parts, heat shields, cookware fittings.Information provided by Bak AGBak AG became a p..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 38110 Phenolic Formaldehyde Resin, High Surface Quality  (discontinued **)
Phenolic molding compound, mainly organically filled.Application areas: Devices for the electrical installation, pan handles, knobs, mainly for compression molding.Information provided by Bak AGBak ..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information..
Charpy Impact, Notched 0.140 J/cm²
0.666 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® Frost 952 51 Acrylic Polymer
Information provided by Lucite International
Charpy Impact, Notched 0.140 J/cm²
0.666 ft-lb/in²
LATI Latigea B01 F1 Bio-Polymer
Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr..
Charpy Impact, Notched 0.140 J/cm²
0.666 ft-lb/in²
ISO 179-1
Vyncolit TX10916/15 Graphite Filled Novolac Phenolic
Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is requiredInformation provided by Sumitomo Bak North America, Inc.
Charpy Impact, Notched 0.140 J/cm²
0.666 ft-lb/in²
DIN 53453
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to ..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed &n
Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed &nbs
Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol..
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed
Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou..
Copyright © lookpolymers.com All Rights Reserved