Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.0300 - 0.600 J/cm² @Temperature -30.0 - -20.0 °C |
0.143 - 2.86 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.289 J/cm² Grade Count:43 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Charpy Impact, Notched | 0.0300 - 2.00 J/cm² @Temperature -30.0 - -20.0 °C |
0.143 - 9.52 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.413 J/cm² Grade Count:58 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |