Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.610 J/cm²

@Temperature -30.0 °C
2.90 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 131E-28 Cellulose Acetate  (discontinued **)
28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 0.610 - 2.00 J/cm²

@Temperature -30.0 - -20.0 °C
2.90 - 9.52 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 1.17 J/cm² Grade Count:30
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Charpy Impact, Notched 0.610 J/cm²
2.90 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Charpy Impact, Notched 0.610 J/cm²
2.90 ft-lb/in²
ISO 179/1eA
Polyplastics FR-PET® BN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
Information provided by PolyPlastics.
Charpy Impact, Notched 0.610 J/cm²
2.90 ft-lb/in²
ISO 179/1eA
Polyplastics FR-PET® CN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
Information provided by PolyPlastics.
Charpy Impact, Notched 0.609 J/cm²

@Temperature 22.8 °C
2.90 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CMU 308 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed with good stiffness/toughness balance fro electrical appliance such as washing machine and dryer stands.Availability: Africa ..
Charpy Impact, Notched 0.610 J/cm²
2.90 ft-lb/in²
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Conditioned)
Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V..
Charpy Impact, Notched 0.610 J/cm²
2.90 ft-lb/in²
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned)
Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent...
Charpy Impact, Notched 0.610 J/cm²

@Temperature -30.0 °C
2.90 ft-lb/in²

@Temperature -22.0 °F
ISO data
BASF Capron® HPN 9315G Impact Modified, 15% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9315G is a 15% glass reinforced, impact modified polyamide 6 injection molding grade resin in the High Productivity Nylon Series developed for applications requiring superior dry-as-molde..
Charpy Impact, Notched 0.610 J/cm²

@Temperature -20.0 °C
2.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound
Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance..
Charpy Impact, Notched 0.610 J/cm²
2.90 ft-lb/in²
ASTM D256
Plenco 1581 Polyester, Briquette, Transfer Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..
Charpy Impact, Notched 0.610 J/cm²
2.90 ft-lb/in²
ISO 179/1eA
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..