Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 20.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 20.0 MPa
>= 2900 psi
Chip Bonding
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative
NanoTach® is a thick paste of nano-sized silver powder in an organic binder that can be used as an alternative to solder or epoxy in semiconductor devices in the state-of-the-art individual package..
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Brass, Shear; ISO 4587
Permabond 170 Cyanoacrylate, gap filling
PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w..
Adhesive Bond Strength 20.0 - 24.0 MPa
2900 - 3480 psi
Steel, Shear; ISO 4587
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Steel, Shear; ISO 4587
Permabond 268 Cyanoacrylate, General purpose
PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyano..
Adhesive Bond Strength 20.0 - 35.0 MPa
2900 - 5080 psi
Steel , Shear; ISO 4587
Permabond ES562 Epoxy Resin
PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t..
Adhesive Bond Strength 20.0 - 30.0 MPa
2900 - 4350 psi
Mild steel, Shear; ISO 4587
Permabond ET5401 Epoxy Resin
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..
Adhesive Bond Strength 20.0 MPa
2900 psi
steel collar and pin shear; ISO 10123
Permabond HM165 Anaerobic Retainer
Permabond® HM165 is a high viscosity anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It is best suited for cylindrical parts and where high temperatu..
Adhesive Bond Strength 20.0 - 25.0 MPa
2900 - 3630 psi
Steel, Shear
Permabond TA439 Toughened Acrylic Adhesive
Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f..
Adhesive Bond Strength 20.0 - 25.0 MPa
2900 - 3630 psi
Steel/steel after 24 hours, Shear
Permabond TA459 Toughened Acrylic Adhesive
Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens..
Adhesive Bond Strength 20.0 - 25.0 MPa
2900 - 3630 psi
Steel/steel after 24 hours, Shear
Permabond TA4590 Toughened Acrylic Adhesive
Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen..
Adhesive Bond Strength 20.0 - 25.0 MPa
2900 - 3630 psi
Mild steel, Shear
Permabond TA4592 Toughened Acrylic Adhesive
PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt..
Adhesive Bond Strength 20.0 MPa
2900 psi
Steel lap shear
Resinlab® CYNERGY CA6604 Adhesive
Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a ..
Adhesive Bond Strength 20.0 MPa
2900 psi
Steel lap shear
Resinlab® CYNERGY CA6605 Adhesive
Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a ..
Adhesive Bond Strength 20.0 MPa
2900 psi
Steel lap shear
Resinlab® CYNERGY CA6704 Adhesive
Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal ..
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Steel, Shear; ISO 4587
Permabond 108 Cyanoacrylate, gap filling
PERMABOND® 108 is an intermediate viscosity cyanoacrylate that is used to bond through intermediate gaps. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate adhes..
Adhesive Bond Strength 20.0 MPa
2900 psi
Grit blasted Steel, Shear
Permabond 260 Cyanoacrylate
PERMABOND 260 is a low viscosity cyanoacrylate ideal for wicking type application. PERMABOND 260 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates..
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Steel, Shear; ISO 4587
Permabond 799 Cyanoacrylate, Surface insensitive
PERMABOND® 799 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cu..
Adhesive Bond Strength 20.0 MPa
2900 psi
Steel lap shear
Resinlab® CYNERGY CA6603 Adhesive
Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a ..
Adhesive Bond Strength 20.0 MPa
2900 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 224-1 Rapid Room Temperature Cure Epoxy Adhesive
TRA-BOND 224-1 room temperature curing epoxy adhesive develops structural strength rapidly. Unlike most "rapid cure" epoxies which gel in one or two minutes, TRA-BOND 224-1 adhesive exhibits a 30 mi..
Adhesive Bond Strength 20.0 MPa
2900 psi
Lap shear, alum to alum, 1 hr @ 100°C
Tra-Con Tra-Bond 526M01 Rigid Thixotropic Adhesive
TRA-BOND 526M01 is two-component, rigid, thixotropic material developed specifically for fiber optic applications. The material is a cream color when mixed and changes to a red amber color when full..
Adhesive Bond Strength 20.0 MPa
2900 psi
Lap shear, alum to alum
Tra-Con Tra-Bond F123NC High Temperature Fiber Optic Epoxy Adhesive
TRA-BOND F123 NC is a fast cure, low viscosity, two-component epoxy formulation for bonding fiber optic bundles, potting glass fibers, and/or terminating single or multi-channel fiber optic connecto..
Adhesive Bond Strength 20.0 MPa
2900 psi
Lap shear, alum to alum
Tra-Con Tra-Bond F125 Fast Gel Clear Epoxy Adhesive
TRA-BOND F125 is a 10 minute gelling epoxy recommended for use in fiber optic connectors, optical and industrial bonding applications. This clear, two part system is easily mixed and used at room te..
Adhesive Bond Strength 20.0 MPa
2900 psi
Grit blasted steel
Loctite® 420 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Adhesive Bond Strength 20.0 MPa
2900 psi
Bond strength to dentin using 3M Single Bond adhesive; C2 color
3M Filtek™ P60 Posterior Restorative Dental Composite
Filtek P60 posterior restorative is an esthetic, light cured, radiopaque composite specifically designed for use in posterior direct or indirect restorations. Bonding to tooth structure is accompli..
Adhesive Bond Strength 20.0 MPa

@Temperature -54.4 °C
2900 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-2/W Epoxy Adhesive
This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac..
Adhesive Bond Strength 20.0 MPa

@Temperature 82.2 °C
2900 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
Armstrong A-40 Epoxy Adhesive
Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re..
Adhesive Bond Strength 20.0 MPa
2900 psi
alum to alum
Atom Adhesives AA-BOND F123 Epoxy Adhesive
AA-BOND F123 is a low viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating single or multi..
Adhesive Bond Strength 20.0 MPa
2900 psi
alum to alum
Atom Adhesives AA-BOND F123BK Epoxy Adhesive
AA-BOND F123BK is a low viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating single or mul..
Adhesive Bond Strength 20.0 MPa
2900 psi
alum to alum
Atom Adhesives AA-BOND F125 Epoxy Adhesive
AA-BOND F125 is a 8 minutes gelling epoxy recommended for use in fiber optic connectors, optical and industrial bonding applications. AA-BOND F125 is clear, two part system is easily mixed and used ..
Adhesive Bond Strength 20.0 MPa
2900 psi
Grit blasted Steel, Shear
Permabond 262 Cyanoacrylate
PERMABOND 262 is a low viscosity cyanoacrylate ideal for wicking type application. PERMABOND 262 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates..