Mechanical Properties Metric English Comments
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
Steel, Shear; ISO 4587
Permabond 105 Cyanoacrylate, for difficult rubbers
PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives..
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Brass, Shear; ISO 4587
Permabond 170 Cyanoacrylate, gap filling
PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w..
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Stainless Steel, Shear; ISO 4587
Permabond 170 Cyanoacrylate, gap filling
PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w..
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Steel, Shear; ISO 4587
Permabond 268 Cyanoacrylate, General purpose
PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyano..
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
ISO 4587, Shear
Permabond 790 Cyanoacrylate, Surface insensitive
PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar..
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Mild steel, Shear
Permabond TA4300 Toughened Acrylic Adhesive
PERMABOND® TA4300 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue...
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Steel, Shear; ISO 4587
Permabond 108 Cyanoacrylate, gap filling
PERMABOND® 108 is an intermediate viscosity cyanoacrylate that is used to bond through intermediate gaps. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate adhes..
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
ISO 4587, Shear
Permabond 791 Cyanoacrylate, Surface insensitive
PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar..
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
Steel, Shear; ISO 4587
Permabond 795 Cyanoacrylate, Surface insensitive
PERMABOND® 795 is a moderate viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastome..
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Steel, Shear; ISO 4587
Permabond 799 Cyanoacrylate, Surface insensitive
PERMABOND® 799 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cu..
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Steel, Shear; ISO 4587
Permabond 919 Cyanoacrylate, High temperature
Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I..
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
ISO 4587, Shear
Permabond 792 Cyanoacrylate, Surface insensitive
PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar..