Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Permabond ET5401 Epoxy Resin

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Permabond
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond ET5401 Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET5401 forms tough bonds providing high peel resistance and high shear strength coupled with excellent resistance to high temperatures. ET5401 performance is enhanced by curing at high temperature or being exposed to high temperature (such as during paint-stoving). Features & Benefits: Adhesion to a wide variety of substrates Full cure at room temperature Easy to apply High shear and peel strength Good impact strength High temperature resistance Non-drip rheology Information provided by Permabond.
Physical Properties Metric English Comments
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 75
65 - 75
Cured at 25°C
75 - 85
75 - 85
Cured for 1 hr at 80°C
Adhesive Bond Strength 6.00 - 8.00 MPa
870 - 1160 psi
FRP Glass Polyester, Shear; ISO 4587
10.0 - 15.0 MPa
1450 - 2180 psi
Grit blasted mild steel, Shear; ISO 4587
19.0 - 23.0 MPa
2760 - 3340 psi
FRP Glass Epoxy, Shear; ISO 4587
22.0 - 24.0 MPa
3190 - 3480 psi
Carbon Fiber, Shear; ISO 4587
20.0 - 30.0 MPa
2900 - 4350 psi
Mild steel, Shear; ISO 4587
Peel Strength 5.60 - 6.40 kN/m
32.0 - 36.5 pli
Cured for 1 hr at 80°C
10.0 - 12.0 kN/m
57.1 - 68.5 pli
Cured for 15 mins at 200°C
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 80.0 °C
1.00 hour

@Temperature 176 °F
full cure
180 - 240 min

@Temperature 25.0 °C
3.00 - 4.00 hour

@Temperature 77.0 °F
handling time
5760 - 10100 min

@Temperature 25.0 °C
96.0 - 168 hour

@Temperature 77.0 °F
full cure
Pot Life 10.0 - 12.0 min

@Temperature 25.0 °C
10.0 - 12.0 min

@Temperature 77.0 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Black for Polyamine Hardener
White for Epoxy Resin
Maximum Gap Fill (mm) 5
Strength Retention 100% at 0°C
Relative to 0°C
15% at 150°C
Relative to 0°C
80% at 100°C
Relative to 0°C
90% at 50°C
Relative to 0°C
Users viewing this material also viewed the following: