Polymer Property : Adhesive Bond Strength = 3630 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 23.0 - 25.0 MPa
3340 - 3630 psi
Steel, Shear; ISO 4587
Permabond 170 Cyanoacrylate, gap filling
PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w..
Adhesive Bond Strength 15.0 - 25.0 MPa
2180 - 3630 psi
Mild steel, Shear
Permabond TA430 Acrylic Adhesive & Initiator
PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin..
Adhesive Bond Strength 15.0 - 25.0 MPa
2180 - 3630 psi
Mild steel, Shear
Permabond TA435 Toughened Acrylic Adhesive & Initiator
PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli..
Adhesive Bond Strength 15.0 - 25.0 MPa
2180 - 3630 psi
Mild steel, Shear
Permabond TA436 Toughened Acrylic Adhesive
PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength..
Adhesive Bond Strength 20.0 - 25.0 MPa
2900 - 3630 psi
Steel, Shear
Permabond TA439 Toughened Acrylic Adhesive
Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f..
Adhesive Bond Strength 15.0 - 25.0 MPa
2180 - 3630 psi
Mild steel, Shear
Permabond TA440 Toughened Acrylic Adhesive
PERMABOND TA440 is a two component structural acrylic adhesive suitable for bonding metals, glass, wood, ferrites, ceramics and some rigid plastics. This adhesive may be used in a variety of structu..
Adhesive Bond Strength 20.0 - 25.0 MPa
2900 - 3630 psi
Steel/steel after 24 hours, Shear
Permabond TA459 Toughened Acrylic Adhesive
Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens..
Adhesive Bond Strength 20.0 - 25.0 MPa
2900 - 3630 psi
Steel/steel after 24 hours, Shear
Permabond TA4590 Toughened Acrylic Adhesive
Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen..
Adhesive Bond Strength 20.0 - 25.0 MPa
2900 - 3630 psi
Mild steel, Shear
Permabond TA4592 Toughened Acrylic Adhesive
PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt..
Adhesive Bond Strength 21.0 - 25.0 MPa
3050 - 3630 psi
Steel, Shear; ISO 4587
Permabond 240 Cyanoacrylate, gap filling
PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate..
Adhesive Bond Strength 22.0 - 25.0 MPa
3190 - 3630 psi
Mild steel, Shear
Permabond TA4302 Toughened Acrylic Adhesive
PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..