Permabond 919 Cyanoacrylate, High temperature

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond 919 Cyanoacrylate, High temperature.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMABOND 919 will cure to fixture strength in 10 seconds on most surfaces, and rapidly develops high strength with full cure obtained in 24 hours. The adhesive was specifically designed to meet the high temperature resistance required by certain applications. It provides excellent bond strength to steel, aluminum, and most metal surfaces. The cyanoacrylate will also adhere well to a wide variety of other materials including most types of plastic and rubber. In order to withstand high temperature environments, PERMABOND 919 was designed with a secondary curing mechanism that is activated at temperatures higher than 150°C (302°F). The procedure to activate this mechanism is as follows: 1) Parts are bonded and clamped at room temperature for four hours. 2) The clamped parts are then heated at 150°C (302°F) for two hours. 3) After the two hours, the bond will be thermally resistant up to 250°C (482°).Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 2.0 - 6.0 cP

@Temperature 25.0 °C
2.0 - 6.0 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ISO 868
Adhesive Bond Strength 2.00 MPa
290 psi
Gum rubber, Shear; ISO 4587
3.50 MPa
508 psi
Polystyrene, Shear; ISO 4587
4.00 MPa
580 psi
ABS, Shear; ISO 4587
4.00 MPa
580 psi
Valox, Shear; ISO 4587
7.00 MPa
1020 psi
PC, Shear; ISO 4587
14.0 MPa
2030 psi
Phenolic, Shear; ISO 4587
16.0 - 18.0 MPa
2320 - 2610 psi
Aluminum, Shear; ISO 4587
20.0 - 22.0 MPa
2900 - 3190 psi
Steel, Shear; ISO 4587
Impact 3.0 - 5.0
3.0 - 5.0
kJ/m<sup>2</sup> Adhesive Impact Strength; ASTM D950
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Cure Time <= 0.250 min
<= 0.00417 hour
NBR Rubber, handling time
<= 0.333 min
<= 0.00556 hour
Buna N Rubber, handling time
<= 0.333 min
<= 0.00556 hour
Phenolic, handling time
<= 0.333 min
<= 0.00556 hour
Steel, handling time
1440 min
24.0 hour
full strength
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Maximum Gap Fill (mm) 0.05
Strength Retention 30% at 250°C
Relative to 0°C
60% at 150°C
Relative to 0°C
75% at -50°C
Relative to 0°C
90% at 50°C
Relative to 0°C
Copyright © lookpolymers.com All Rights Reserved