Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 23.0 - 25.0 MPa | 3340 - 3630 psi | Steel, Shear; ISO 4587 |
Permabond 170 Cyanoacrylate, gap filling PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w.. |
|||
Adhesive Bond Strength | 15.0 - 25.0 MPa | 2180 - 3630 psi | Mild steel, Shear |
Permabond TA430 Acrylic Adhesive & Initiator PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin.. |
|||
Adhesive Bond Strength | 15.0 - 25.0 MPa | 2180 - 3630 psi | Mild steel, Shear |
Permabond TA435 Toughened Acrylic Adhesive & Initiator PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli.. |
|||
Adhesive Bond Strength | 15.0 - 25.0 MPa | 2180 - 3630 psi | Mild steel, Shear |
Permabond TA436 Toughened Acrylic Adhesive PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength.. |
|||
Adhesive Bond Strength | 20.0 - 25.0 MPa | 2900 - 3630 psi | Steel, Shear |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Adhesive Bond Strength | 15.0 - 25.0 MPa | 2180 - 3630 psi | Mild steel, Shear |
Permabond TA440 Toughened Acrylic Adhesive PERMABOND TA440 is a two component structural acrylic adhesive suitable for bonding metals, glass, wood, ferrites, ceramics and some rigid plastics. This adhesive may be used in a variety of structu.. |
|||
Adhesive Bond Strength | 20.0 - 25.0 MPa | 2900 - 3630 psi | Steel/steel after 24 hours, Shear |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Adhesive Bond Strength | 20.0 - 25.0 MPa | 2900 - 3630 psi | Steel/steel after 24 hours, Shear |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Adhesive Bond Strength | 20.0 - 25.0 MPa | 2900 - 3630 psi | Mild steel, Shear |
Permabond TA4592 Toughened Acrylic Adhesive PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt.. |
|||
Adhesive Bond Strength | 21.0 - 25.0 MPa | 3050 - 3630 psi | Steel, Shear; ISO 4587 |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Adhesive Bond Strength | 22.0 - 25.0 MPa | 3190 - 3630 psi | Mild steel, Shear |
Permabond TA4302 Toughened Acrylic Adhesive PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |