Atom Adhesives AA-BOND F125 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-BOND F125 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AA-BOND F125 is a 8 minutes gelling epoxy recommended for use in fiber optic connectors, optical and industrial bonding applications. AA-BOND F125 is clear, two part system is easily mixed and used at room temperature. Fiber optic connectors can be polished in as little as 15 to 20 minutes for piston free assurance. The high bond strength of AA-BOND F125 to glass, plastics, ceramics, metals and masonry allows it to be used in a wide array of applications including lens bonding, connector backfills, construction, component assembly and maintenance repair. AA-BOND F125 is low shrinkage epoxy, develops significant properties 1 hour after mixing. However, an extended cure of 4-6 hours at 25°C is required for fully matured bonds.Appearance: Clear Cure Type: Heat cure or Room TemperatureBenefits:Low viscosityFast cureLow Shrinkage Mix Ratio by weight: 100:93/Resin:Hardener Typical Application: Fiber optic assembly, multimode and single mode connectors, small potting and sealing applicationsInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
uncured
Solids Content 100 %
100 %
uncured
Viscosity 9000 cP
9000 cP
Resin, uncured
14000 cP
14000 cP
Hardener, uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Adhesive Bond Strength 20.0 MPa
2900 psi
alum to alum
Thermal Properties Metric English Comments
CTE, linear 59.9 µm/m-°C
33.3 µin/in-°F
Maximum Service Temperature, Air 115 °C
239 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 40.0 °C
104 °F
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+11 ohm-cm
5.00e+11 ohm-cm
Dielectric Constant 4.8

@Frequency 1000 Hz
4.8

@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm
410 kV/in
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 60.0 °C
1.00 hour

@Temperature 140 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 5.00 min
5.00 min
uncured
Descriptive Properties Value Comments
Thixotropic Index 1