Permabond 108 Cyanoacrylate, gap filling

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond 108 Cyanoacrylate, gap filling.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERMABOND® 108 is an intermediate viscosity cyanoacrylate that is used to bond through intermediate gaps. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND cyanoacrylates the ideal adhesives for high speed production lines. Features & Benefits: Fast-setting Some gap fill ability Ideal for automated dispensing Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 400 - 600 cP

@Temperature 25.0 °C
400 - 600 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ISO 868
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Steel, Shear; ISO 4587
Impact 3.0 - 5.0
3.0 - 5.0
kJ/m<sup>2</sup> Adhesive Impact Strength; ASTM D950
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 82.2 °C
180 °F
Minimum Service Temperature, Air -62.2 °C
-80.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Frequency 10000 Hz
2.5

@Frequency 10000 Hz
Dielectric Strength 25.0 kV/mm
635 kV/in
Processing Properties Metric English Comments
Cure Time 0.167 min
0.00278 hour
Steel, handling time
0.167 min
0.00278 hour
Buna N Rubber, handling time
0.167 min
0.00278 hour
Phenolic, handling time
1440 min
24.0 hour
full strength
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Maximum Gap Fill (mm) 0.25
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
55% at -50°C
Relative to 0°C
90% at 50°C
Relative to 0°C