Permabond 268 Cyanoacrylate, General purpose

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond 268 Cyanoacrylate, General purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates. The adhesive bonds to a wide range of substrates including metals, ceramics, plastics and elastomers. It is excellent for bonding difficult-to-bond plastics such as polyacetals. It can also be used on passivated metal surfaces. Features & Benefits: Versatile and general purpose Good gap fill ability Instant setting Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 1200 - 2400 cP

@Temperature 25.0 °C
1200 - 2400 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ISO 868
Adhesive Bond Strength 20.0 - 22.0 MPa
2900 - 3190 psi
Steel, Shear; ISO 4587
Impact 3.0 - 5.0
3.0 - 5.0
kJ/m<sup>2</sup> Adhesive Impact Strength; ASTM D950
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 82.2 °C
180 °F
Minimum Service Temperature, Air -62.2 °C
-80.0 °F
Processing Properties Metric English Comments
Cure Time 0.0833 - 0.167 min
0.00139 - 0.00278 hour
Steel, handling time
0.0833 - 0.167 min
0.00139 - 0.00278 hour
Buna N Rubber, handling time
0.0833 - 0.167 min
0.00139 - 0.00278 hour
Phenolic, handling time
1440 min
24.0 hour
full strength
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Maximum Gap Fill (mm) 0.43
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
55% at -50°C
Relative to 0°C
90% at 50°C
Relative to 0°C