Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Time 86400 sec |
0.012 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Thickness 3.20 mm |
0.012 - 0.014 in/in @Thickness 0.126 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm @Thickness 3.17 mm |
0.012 - 0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000MDHL Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedForm: Pellets Information provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.020 cm/cm @Thickness 3.20 mm |
0.012 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® HV1005S PBT Description: Injection Molding, PBT, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 1.00 mm |
0.012 in/in @Thickness 0.0394 in |
|
Kuraray Genestarâ„¢ TA104 Nylon Reinforced injection grade.Main Features:High reflectivityLess color change by heat and lightHigh reliabilityExample of applications:LED reflectors |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-220 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latistat 66-06 PA66 Dissipative product based on Polyamide 66 (PA66). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 2.00 mm |
0.012 in/in @Thickness 0.0787 in |
ASTM D955 |
Lavergne VYPET PBT 6300 BK PBT Unreinforced, Impact Modified Vypet PBT 6300 BK is an unreinforced PBT injection molding compound offering excellent dimensional stability, chemical resistance, low moisture absorption and good electrical properties.Features: Hi.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | |
Solvay TECHNYL® PSB 286 PA6, DRY Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RZL36 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RZL36 is a compound based on PA 66 resin containing Milled Glass, PTFE. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA (Asia Pacific) LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® PA6/6 C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm | 0.012 - 0.014 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics ULTEM SILTEM-STM1500 PEI (Europe-Africa-Middle East) SILTEM STM1500 is a flexible siloxane-polyetherimide copolymer for cable and wire coatings. RoHS compliant. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® HDPE TM40 40% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6 E M/SL4 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant and Silicone LubricantFeatures: Low Friction, Good Wear Resistance and LubricatedAppearance: BlackInformation provid.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.019 cm/cm @Thickness 3.20 mm |
0.012 - 0.019 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm | 0.012 - 0.018 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSS/4 PA666 Product description: Grilon TSS/4 is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/4 has the following important properties: Good flow behaviorEas.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 2.00 mm |
0.012 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 5533 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 7033 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 7233 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7233 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm @Thickness 3.17 mm |
0.012 - 0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000MD5L Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant (5%)Features: LubricatedForm: Pellets Information provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latimass 52/11-01 D020 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers TPB-125 Polybutylene Terephthalate, 25% Mineral Reinforced Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |