Polymer Property : Linear Mold Shrinkage, Flow = 0.020 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
PolyOne LubriOne™ GF-1010 40 MS 2 HS Black 37 Polyamide 6 (Nylon 6)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Linear Mold Shrinkage, Flow 0.011 - 0.020 cm/cm
0.011 - 0.020 in/in
ASTM D955
PolyOne Maxxam™ FR PP 402 Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
Linear Mold Shrinkage, Flow 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
ASTM D955
PolyOne Versaflex™ HC MT222 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT222 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT222 has been specially formulated without the use of any plasticize..
Linear Mold Shrinkage, Flow 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
ASTM D955
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Linear Mold Shrinkage, Flow 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
ASTM D955
PolyOne Versalloy™ XL 9070-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9070-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ASTM D955
Celanese Celanex® 1700A PBT  (Unverified Data**)
Celanex 1700A is a very high molecular weight grade of unreinforce polybutylene terephthalate for extrusion applications.Highest molecular weightInformation provided by Celanese
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ISO 294-4
Celanese Celanex® 1700A PBT  (Unverified Data**)
Celanex 1700A is a very high molecular weight grade of unreinforce polybutylene terephthalate for extrusion applications.Highest molecular weightInformation provided by Celanese
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ASTM D955
Celanese Celanex® 2001 PBT  (Unverified Data**)
Celanex 2001 is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications. Celanex 2001 exhibits the high melt st..
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ASTM D955
Celanese Celanex® 2003HR PBT  (Unverified Data**)
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityHydrolytically stable / injectionInformation provided b..
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ASTM D955
Celanese Celanex® 2104UV PBT, UV Resistant  (Unverified Data**)
Celanex 2104UV is an unreiforced, impact modified, UV stabilized PBT designed for outdoor agricultural, industrial and automotive applications. Celanex 2104UV is suitable for injection molding appli..
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ISO 294-4
Celanese Celanex® 2404 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2404 MT Natural is an unreinforced PTFE filled PBT with improved friction, sliding, and wear properties that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administra..
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ASTM D955 and ISO 294-4
Ravago Manufacturing Americas Hylon® N1200HL BK Nylon 6/6  (discontinued **)
Available in North AmericaAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedAuto Specifications: DELPHI QMPL-1257 Color: BlackForm: PelletsInformation provided by Rava..
Linear Mold Shrinkage, Flow 0.017 - 0.020 cm/cm

@Thickness 3.20 mm
0.017 - 0.020 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUCEL HI520 POM+Rubber, High Impact
Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.012 - 0.020 cm/cm

@Thickness 3.20 mm
0.012 - 0.020 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® GP1006FD PBT
Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica..
Linear Mold Shrinkage, Flow 0.012 - 0.020 cm/cm

@Thickness 3.20 mm
0.012 - 0.020 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® HV1005S PBT
Description: Injection Molding, PBT, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.015 - 0.020 cm/cm

@Thickness 3.20 mm
0.015 - 0.020 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® HX215HP PBT
High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta..
Linear Mold Shrinkage, Flow 0.0080 - 0.020 cm/cm
0.0080 - 0.020 in/in
ASTM D955
Shinkong Synthetic Fibers Shinite® T101 PET
Information from Shinkong Synthetic Fibers Corp.
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Europe-Africa-Middle East)
NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance.
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ISO DIS 294-4
Wellman Wellamid® 21LH-NBK4 General Purpose Nylon 66
Description: General Purpose Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ISO DIS 294-4
Wellman Wellamid® MRT1487 BK 32% Mineral Reinforced, Toughened Grade Nylon 66
Description: Mineral Reinforced, Toughened Grade Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
DIS 294-4
Wellman Wellamid® MRT1487 N Nylon 66, 32% Mineral Reinforced, Impact Modified
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Flow 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
Elastocon TPE Technologies Elastocon® 8078N Thermoplastic Elastomer
Elastocon® 8078N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078N is FDA compliant and well suited..
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
on Tensile Bar; E2P method
Eurostar Staramide A28 PA66, Injection Molding
Staramide A28 is an Unreinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
on Tensile Bar; E2P method
Eurostar Staramide A28N PA66, Nucleated, Injection Molding
Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
on Tensile Bar; E2P method
Eurostar Staramide A40 PA66, Extrusion
Staramide A40 is Unreinforced, High Viscosity Polyamide 66, Extrusion ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
ASTM D955
Clariant Renol 6601L Nylon 66, Lubricated
Data provided by Clariant Masterbatches
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ISO 294-4
Celanese Celanex® 2003-2 PBT, Unfilled
Celanex 2003-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability, and good flow characterictics. Celanex 2003-2 is a medium h..
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ISO 294-4
Celanese Celanex® 2002UV PBT, Unfilled
Celanex 2002UV is a general purpose,unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability and UV resistance. Celanex 2002UV is a medium flow materialTo..
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ASTM D955
Celanese Celanex® 2003-3 PBT, Unfilled
Celanex 2003-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability, and good flow characterictics. Celanex 2003-3 is a medium h..
Linear Mold Shrinkage, Flow 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
PolyOne LubriOne™ ATH-000/10T 2S Acetal (POM) Homopolymer  (discontinued **)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..