Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ASTM D955 |
PolyOne Maxxam™ MD 4245-1000 Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ASTM D955 |
PolyOne Maxxam™ MD 4245-59770 Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ASTM D955 |
PolyOne Maxxam™ PPC-20C Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm @Thickness 4.00 mm, Temperature 23.0 °C |
0.010 - 0.015 in/in @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded, Bergmann Method; ASTM D955 |
PolyOne Bergamid™ B70 GK/Mi30 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm | 0.013 - 0.015 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B80MB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.015 cm/cm @Thickness 3.20 mm |
0.0070 - 0.015 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® SG3180S PBT+PET+MF18% Description: Injection Molding, PBT+PET+MF18%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity i.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | |
LATI Latigray 52/11-01 CX/70 PP Homopolymer Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | |
LATI Latilub 45/7-20T HDPE, PTFE Reinforced Self-lubricating product based on High density polyethylene (HD-PE). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latilub 66-02S PA66, Silicone Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latishield 66-10A PA66, Steel Fiber Reinforced EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.015 cm/cm | 0.0050 - 0.015 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Stat-kon ZX05043 PPE+PS (Europe-Africa-Middle East) LNP* Stat-kon* ZX05043 is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE, Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm @Time 86400 sec |
0.011 - 0.015 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOTUF R1000I PA 66 (Asia Pacific) High Impact Nylon 66 compound containing Impact Modifier. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm @Time 86400 sec |
0.011 - 0.015 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf R1000IX4 PA 66 (Europe-Africa-Middle East) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | annealed 130C 1hr; ASTM D955 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific) Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm @Thickness 3.20 mm |
0.013 - 0.015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Staramide B28H PA6, Heat Stabilized, Injection Molded Staramide B28H is a Heat Stabilized, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Staramide B28N PA6, Nucleated, Injection Molded Staramide B28N is a Nucleated and Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Staramide B40 PA6, Extrusion Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm @Time 86400 sec |
0.011 - 0.015 in/in @Time 24.0 hour |
ISO 294 |
Eurostar Staramide R1000IX4 PA66, Impact Modified, Injection Molded Staramide R1000IX4 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI020 Star X 1020)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Starflam AFR200B PA66, Flame Retardant, Injection Molding Staramide AFR200B is an Unfilled, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm @Time 86400 sec |
0.013 - 0.015 in/in @Time 24.0 hour |
E2P method |
Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRB40K004-WT1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latimass 52/11-01 D020 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | |
Solvay TECHNYL® 1011R PA6, DRY Description: Polyamide 6, Unfilled, lubricated, for injection molding. Available in: Asia Pacific Product Applications: TECHNYL® 1011R is used in all sectors of industry, offering an excellent flow.. |