SABIC Innovative Plastics LNP LUBRICOMP RZL36 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RZL36 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* RZL36 is a compound based on PA 66 resin containing Milled Glass, PTFE. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.012 cm/cm
0.012 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
5 mm/min; ISO 527
Elongation at Yield 2.1 %
2.1 %
5 mm/min; ISO 527
Tensile Modulus 4.80 GPa
696 ksi
1 mm/min; ISO 527
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
Flexural Modulus 4.30 GPa
624 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 53.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
29.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af