Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shinkong Synthetic Fibers Shinite® N602 Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Shinkong Synthetic Fibers Corp
Trade Name Shinite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinite® N602 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Water Absorption 1.1 %
1.1 %
ASTM D570
Linear Mold Shrinkage, Flow 0.012 - 0.018 cm/cm
0.012 - 0.018 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Yield Strength 83.4 MPa
12100 psi
ASTM D790
Flexural Modulus 2.65 GPa
384 ksi
ASTM D790
Izod Impact, Notched 0.392 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.735 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 V-0
V-0
Users viewing this material also viewed the following: