Kuraray Genestarâ„¢ TA104 Nylon

Category Polymer , Thermoplastic , Nylon
Manufacturer Kuraray Company
Trade Name Genestar™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray Genestarâ„¢ TA104 Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reinforced injection grade.Main Features:High reflectivityLess color change by heat and lightHigh reliabilityExample of applications:LED reflectors
Physical Properties Metric English Comments
Specific Gravity 1.61 g/cc
1.61 g/cc
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Thickness 1.00 mm
0.012 in/in

@Thickness 0.0394 in
Linear Mold Shrinkage, Transverse 0.011 cm/cm

@Thickness 1.00 mm
0.011 in/in

@Thickness 0.0394 in
Spiral Flow 5.40 cm

@Load 750 kg,
Temperature 320 °C
2.13 in

@Load 1650 lb,
Temperature 608 °F
0.5mm diameter
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 1.4 %
1.4 %
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 4.50 GPa
653 ksi
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 192 °C
378 °F
ASTM D648
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Descriptive Properties Value Comments
Applications LED Reflectors
Other Features High reflectivity
High reliabaility
Less color change by heat and light