Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0090 - 0.016 cm/cm | 0.0090 - 0.016 in/in | ASTM D955 |
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE) Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.016 cm/cm | 0.0090 - 0.016 in/in | ASTM D955 |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | ASTM D955 |
PolyOne Dynaflex™ G7960-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm @Thickness 0.318 mm |
0.014 - 0.016 in/in @Thickness 0.0125 in |
5" x 0.5" x 0.125"; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | ASTM D955 |
PolyOne Dynaflex™ G7960-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm @Thickness 3.20 mm |
0.013 - 0.016 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUCEL FW720F Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 9002-84-2Information provided by LG.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | |
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | |
LATI Latilub 66-20T PA66, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.016 cm/cm | 0.011 - 0.016 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP MG004 PP (Europe-Africa-Middle East) LNP* Lubricomp* MG004 is a compound based on Polypropylene resin containing Graphite Powder. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.016 cm/cm @Thickness 0.750 - 2.30 mm |
0.0090 - 0.016 in/in @Thickness 0.0295 - 0.0906 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.016 cm/cm @Thickness 0.750 - 2.30 mm |
0.0090 - 0.016 in/in @Thickness 0.0295 - 0.0906 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm @Thickness 3.18 mm |
0.014 - 0.016 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.016 cm/cm @Thickness 3.20 mm |
0.0060 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.016 cm/cm | 0.015 - 0.016 in/in | mold temp=100°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX902E PPE+PA (Europe-Africa-Middle East) NORYL GTX902E is a low cost GTX grade especially developed for automotive (wheel)trims. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm @Thickness 3.20 mm |
0.013 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm @Thickness 3.20 mm |
0.013 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm @Thickness 3.20 mm |
0.013 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX924 PPE+PA (Europe-Africa-Middle East) NORYL GTX 924 is an UV stabilized unfilled Noryl GTX grade with improved processability. Noryl GTX 924 is specially designed for wheeltrim applications. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm @Thickness 3.20 mm |
0.013 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Asia Pacific) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.016 cm/cm | 0.015 - 0.016 in/in | mold temp=100°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Thermocomp RB003 PA 66 (Europe-Africa-Middle East) 15% glass beads filled polyamide 66 injection moulding resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22L-BL Engineering Grade Nylon 66 Description: Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm @Thickness 4.00 mm |
0.014 - 0.016 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide R1000K PA66, Injection Molded Staramide R1000K is an Unreinforced Radiation Crosslinkable Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | on Tensile Bar; E2P method |
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |