Lucent Polymers TPB-125 Polybutylene Terephthalate, 25% Mineral Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Mineral Filled
Manufacturer Lucent Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers TPB-125 Polybutylene Terephthalate, 25% Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Thickness 3.17 mm
0.012 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
ASTM D638
Elongation at Break >= 5.0 %
>= 5.0 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 4.138 GPa
600.2 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.806 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648