Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000100 - 0.00600 cm/cm | 0.000100 - 0.00600 in/in | Average value: 0.00250 cm/cm Grade Count:54 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00600 cm/cm | 0.000 - 0.00600 in/in | Average value: 0.00223 cm/cm Grade Count:50 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00600 cm/cm | 0.00300 - 0.00600 in/in | Average value: 0.00433 cm/cm Grade Count:3 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00359 cm/cm Grade Count:17 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00289 cm/cm Grade Count:35 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00332 cm/cm Grade Count:17 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm @Thickness 3.20 mm |
0.00400 - 0.00600 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company ESD C 201.4 F Nylon 12 (PA) Glass Fiber - Electrically Conductive |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron AN450M Flame Retardant ABS Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21V ABS Injection Molding Grade Super High Gloss, High RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron TIM 200 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21V ABS Injection Molding Grade Super High Gloss, High RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade Electroplating, High FlowInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE45I Extrusion ABS Very High Impact, Low Flow, High Rigidity and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00386 cm/cm Grade Count:7 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00400 cm/cm Grade Count:19 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00313 cm/cm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00253 cm/cm Grade Count:16 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00425 cm/cm Grade Count:4 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00291 cm/cm Grade Count:35 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00280 cm/cm Grade Count:22 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM17V ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21G ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |