Polymer Property : Linear Mold Shrinkage = 0.000100 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000100 - 0.0200 cm/cm
0.000100 - 0.0200 in/in
ASTM D955
Niche Polymer PPHM15BK Homopolymer PP
Information provided by Niche Polymer
Linear Mold Shrinkage 0.000100 - 0.0200 cm/cm
0.000100 - 0.0200 in/in
ASTM D955
Niche Polymer PPHM6BK Homopolymer PP
Information provided by Niche Polymer
Linear Mold Shrinkage 0.000100 - 0.00600 cm/cm
0.000100 - 0.00600 in/in
Average value: 0.00250 cm/cm Grade Count:54
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Linear Mold Shrinkage 0.000100 - 0.00260 cm/cm
0.000100 - 0.00260 in/in
Average value: 0.00117 cm/cm Grade Count:3
Overview of materials for Polystyrene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Wood Filled". Each property range of values reported is minimum and maximum values of appro..
Linear Mold Shrinkage 0.000100 - 0.00300 cm/cm
0.000100 - 0.00300 in/in
Average value: 0.00150 cm/cm Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
Linear Mold Shrinkage 0.000100 - 0.00200 cm/cm
0.000100 - 0.00200 in/in
Average value: 0.000593 cm/cm Grade Count:15
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an..
Linear Mold Shrinkage 0.000100 - 0.0140 cm/cm
0.000100 - 0.0140 in/in
Average value: 0.00727 cm/cm Grade Count:51
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Linear Mold Shrinkage 0.000100 - 0.00400 cm/cm
0.000100 - 0.00400 in/in
Average value: 0.00183 cm/cm Grade Count:6
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage 0.000100 - 0.00400 cm/cm
0.000100 - 0.00400 in/in
Average value: 0.00150 cm/cm Grade Count:17
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Linear Mold Shrinkage 0.000100 - 0.00200 cm/cm
0.000100 - 0.00200 in/in
Average value: 0.000875 cm/cm Grade Count:4
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and..
Linear Mold Shrinkage 0.000100 - 0.00600 cm/cm
0.000100 - 0.00600 in/in
Average value: 0.00178 cm/cm Grade Count:10
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma..
Linear Mold Shrinkage 0.000100 - 0.0100 cm/cm
0.000100 - 0.0100 in/in
Average value: 0.00414 cm/cm Grade Count:227
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Linear Mold Shrinkage 0.000100 - 0.0500 cm/cm
0.000100 - 0.0500 in/in
Average value: 0.0144 cm/cm Grade Count:176
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.000100 - 0.0350 cm/cm
0.000100 - 0.0350 in/in
Average value: 0.0127 cm/cm Grade Count:220
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..