Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00300 - 0.00600 cm/cm | 0.00300 - 0.00600 in/in | Average value: 0.00433 cm/cm Grade Count:3 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00277 cm/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00600 cm/cm | 0.000500 - 0.00600 in/in | Average value: 0.00180 cm/cm Grade Count:27 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00468 cm/cm Grade Count:11 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00600 cm/cm | 0.000500 - 0.00600 in/in | Average value: 0.00240 cm/cm Grade Count:29 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00600 cm/cm | 0.000 - 0.00600 in/in | Average value: 0.00210 cm/cm Grade Count:18 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00332 cm/cm Grade Count:17 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron TIM 200 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron TIM 300 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron TIM 200 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21G ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE45I Extrusion ABS Very High Impact, Low Flow, High Rigidity and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron TIM 300 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00386 cm/cm Grade Count:7 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00600 cm/cm | 0.000100 - 0.00600 in/in | Average value: 0.00178 cm/cm Grade Count:10 |
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00253 cm/cm Grade Count:16 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00280 cm/cm Grade Count:22 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00400 cm/cm Grade Count:12 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM17V ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade Electroplating, High FlowInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |