Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electroplating, High FlowInformation provided by Bhansali
Physical Properties Metric English Comments
Specific Gravity 1.045 g/cc
1.045 g/cc
ASTM D792
Linear Mold Shrinkage 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
ASTM D955
Melt Flow 43.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
43.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 41.2 MPa

@Thickness 3.20 mm
5970 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 63.7 MPa

@Thickness 6.40 mm
9250 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Flexural Modulus 2.21 GPa

@Thickness 6.40 mm
320 ksi

@Thickness 0.252 in
5 mm/min; ASTM D790
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
2.75 J/cm

@Thickness 3.20 mm
5.14 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C

@Thickness 6.40 mm
199 °F

@Thickness 0.252 in
Method A; ASTM D648
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in