| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
| Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.0500 % | 0.0500 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.20 % | 0.20 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 5.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
| Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 70 | 70 | 4min; ISO 5659-2 |
| Tensile Strength at Break | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
| 58.0 MPa | 8410 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 64.0 MPa | 9280 psi | Type I, 50 mm/min; ASTM D638 |
| 64.0 MPa | 9280 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 8.3 % | 8.3 % | 50 mm/min; ISO 527 |
| 20 % | 20 % | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Yield | 4.6 % | 4.6 % | Type I, 50 mm/min; ASTM D638 |
| 4.7 % | 4.7 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.22 GPa | 322 ksi | 5 mm/min; ASTM D638 |
| 2.44 GPa | 354 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 100 MPa | 14500 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 2.36 GPa | 342 ksi | 2 mm/min; ISO 178 |
| 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
| 1.81 J/cm @Temperature -30.0 °C |
3.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
| 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 52.0 J @Temperature 23.0 °C |
38.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 124 °C | 255 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 122 °C @Thickness 3.20 mm |
252 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D1525 |
| 143 °C | 289 °F | Rate B/50; ISO 306 | |
| 146 °C | 295 °F | Rate B/120; ISO 306 | |
| UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
| UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
UL 94 by SABIC-IP |
| Oxygen Index | 33 % | 33 % | ISO 4589 |
| Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
| 775 °C | 1430 °F | IEC 60695-2-13 | |
| 800 °C | 1470 °F | IEC 60695-2-13 | |
| 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 7.62e+17 ohm-cm | 7.62e+17 ohm-cm | ASTM D257 |
| 7.62e+17 ohm-cm | 7.62e+17 ohm-cm | IEC 60093 | |
| Surface Resistance | 1.25e+18 ohm | 1.25e+18 ohm | ASTM D257 |
| 1.25e+18 ohm | 1.25e+18 ohm | ROA; IEC 60093 | |
| Dielectric Constant | 2.7 @Frequency 1.00e+6 Hz |
2.7 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 2.78 @Frequency 1.00e+6 Hz |
2.78 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| Dielectric Strength | 34.1 kV/mm @Thickness 3.20 mm |
866 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
| 34.1 kV/mm @Thickness 3.20 mm |
866 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 | |
| Dissipation Factor | 0.0029 @Frequency 1.00e+6 Hz |
0.0029 @Frequency 1.00e+6 Hz |
ASTM D150 |
| 0.0029 @Frequency 1.00e+6 Hz |
0.0029 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
| High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| F1 Class Smoke and Toxicity Rating | 3mm | NF F16-101 |
| Flame Spread Index (1.52mm) | 15 | ASTM E 162 |
| Heat Release, MAHRE | 33.6kW/m^2 | ISO 5660-1 |
| Lateral Flame Spread, CFE | 20kW/m^2 | ISO 5658-2 |
| M1 Flame Class Rating | 2mm | NF P 92501 |
| NBS Smoke Density, Flaming, 20 min (3.2 mm) | 120 | ASTM E 662 |
| NBS Smoke Density, Flaming, 4 min (1.52mm) | 30 | ASTM E 662 |
| NBS Smoke Density, Flaming, 4 min (3.2 mm) | 30 | ASTM E 662 |
| NBS Smoke Density, Non-Flaming, 4 min (1.52mm) | 7 | ASTM E 662 |
| Toxicity | 0 | ISO 5659-2 |
| Toxicity (3 mm) | 21.76 | NF X70-100 |