Polymer Property : Izod Impact, Notched = 3.00 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.00 J/cm
<br>@Temperature -30.0 °C
5.62 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
Izod Impact, Notched 3.00 J/cm
<br>@Temperature -30.0 °C
5.62 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific)
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
Izod Impact, Notched 3.00 J/cm
<br>@Temperature -30.0 °C
5.62 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Cycoloy® HCX1640 PC+ABS (Europe-Africa-Middle East)
CYCOLOY™ HCX1640 a PC+ABS blend specially developed for medical devices and pharmaceutical applications requiring improved mechanical performance . It combines good flow with excellent impact and l..
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® RCM6134 PC+ABS (Asia Pacific)
Cycoloy* RCM6134 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1...
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
Radici Heraflex® E 7722 TPC-ET Thermoplastic Elastomer
TPC-ET Thermoplastic Elastomer. High Modulus, Nominal Shore D/15s 69. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.
Izod Impact, Notched 3.00 J/cm
<br>@Temperature 23.0 °C
5.62 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific)
LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci..
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
SABIC BM1052 High Density Polyethylene for Blow Molding
Product Description: BM1052 grade is a high molecular weight High Density Polyethylene copolymer with broad molecular weight distribution. It has excellent processability and exhibits very high im..
Izod Impact, Notched >= 3.00 J/cm
<br>@Temperature 23.0 °C
>= 5.62 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
NIZHNEKAMSKNEFTEKHIM PE 6844G (446H7) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Izod Impact, Notched 3.00 J/cm
<br>@Temperature 23.0 °C
5.62 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East)
LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af..
Izod Impact, Notched 3.00 J/cm
<br>@Temperature 0.000 °C
5.62 ft-lb/in
<br>@Temperature 32.0 °F
ASTM D256
Gichem GIBLEND E45400 Polycarbonate / ABS &nbsp;(discontinued **)
Polycarbonate and ABS blend, high fluidity. Medium Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
Reverse notched; ASTM D256
LG Chemical LUCEL EC-605B Electrically Conductive POM, 5% Carbon Black Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Izod Impact, Notched 3.00 - 4.00 J/cm
<br>@Temperature 23.0 °C
5.62 - 7.49 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
Loxim 500 00HB Polycarbonate/Acrylonitrile Butadiene Styrene
Information provided by Loxim Industries
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific)
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East)
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON UX03320 PPA
LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural.
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL EN7010 PPE+SEBS (Asia Pacific)
High heat, Non halogenated flame retardant Noryl product for Film
Izod Impact, Notched 3.00 J/cm
<br>@Thickness 3.17 mm
5.62 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Unitika P-3001S Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Izod Impact, Notched 3.00 J/cm
<br>@Temperature 23.0 °C
5.62 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram Polytron P60B04 Homopolymer Polypropylene, Chemically Coupled 60% Long Glass Fiber
A CHEMICALLY COUPLED PP 60% LONG GLASS FIBER WITH EXTRA LOAD OF ADDITIVES FOR DILUTION.Information provided by Polyram Ram On Ind.
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM-D256
Polyram RamLloy PJ701 ABS/ASA, General Purpose
PJ 701 IS A GENERAL PURPOSE INJECTION MOLDING ASA& ABS ALLOY . IT HAS GOOD MECHANICAL PROPERTIES SIMILAR TO ABS AND MUCH BETTER WEATHER RESISTANCE. AN IDEAL ECONOMIC CHOICE.Information provided ..
Izod Impact, Notched 3.00 J/cm
<br>@Temperature 23.0 °C
5.62 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram RamShine PV701 ABS, UV Stabilized
UV stabilized ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 3.00 J/cm
<br>@Temperature 23.0 °C
5.62 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram RamShine PV801 ABS, Impact Modified
Impact modified ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 3.00 J/cm
<br>@Temperature 23.0 °C
5.62 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram RamShine PV102 ABS, General Purpose
General purpose ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM-D256
Braskem GP5550BK HDPE High Density Extrusion Polyethylene
GP5550BK is a high-density polyethylene with high molar mass. It is produced with bimodal technology and shows excellent mechanical properties and high resistance to stress cracking. GP5550BK contai..
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM-D256
Braskem PRB 0131 RACO Random Polypropylene Copolymer
PRB 0131 is a low melt flow rate random copolymer with high transparency. This resin is designed for thermoforming, blow molding, and extrusion. This product exhibits excellent processability, low h..
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM 3.2mm
Asahi Kasei Xyron® AT600 Modified Polyphenylene Ether
Applications: Automotive: Body Panels, Mirror Shells, Fuel Door Covers, Hinge Covers, Relay Blocks Electrical and Industrial: Tractor Hoods, Motorcycle Fairings, Yard Maintenance EquipmentInformati..
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX1005X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications.
Izod Impact, Notched 3.00 J/cm
<br>@Temperature 23.0 °C
5.62 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram Polytron A40N02 Nylon 66, 40% Long Fiber
40% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
Braskem BU004 Blow Molding High Density Polyethylene
Containers for lubricating oils, alcohol, cosmetics and yots; Toys.Information provided by Braskem.