| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS
Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance.
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
|
|||
| Izod Impact, Notched (ISO) |
14.0
-
16.0
kJ/m² <br>@Temperature -30.0 - -30.0 °C
|
6.66
-
7.61
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 17.5 kJ/m² Grade Count:4 |
|
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
|
|||
| Izod Impact, Notched (ISO) |
14.0
-
16.0
kJ/m² <br>@Thickness 3.20 - 3.20 mm
|
6.66
-
7.61
ft-lb/in² <br>@Thickness 0.126 - 0.126 in
|
Average value: 17.5 kJ/m² Grade Count:4 |
|
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180 |
|
Iran Petrochemical (PCC) EP-T 30 R Polypropylene
The grade is a medium flow heterophasic the copolymer mainly designed for injection molding application.Application: containers, buckets, pails, crates and also used for automotive parts.Informatio..
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL PX6120 PPE+PS
Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications.
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East)
Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP SFP36 PA12
LNP* LUBRICOMP* SFP36 is a compound based on Nylon 12 resin containing 30% Glass Fiber 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT
LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific)
DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12
LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature 23.0 °C
|
6.66
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP UF009AS PPA (Europe-Africa-Middle East)
LNP* Thermocomp* UF009AS is a compound based on Polyphthalamide resin containing Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP UF009AXP PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF009AXP is a compound based on Polyphthalamide resin containing 45% Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East)
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP DB0049R PC (Europe-Africa-Middle East)
LNP* Thermocomp* DB0049R is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP DF008 PC
LNP THERMOCOMP* DF008 is a compound based on Polycarbonate resin containing 40% Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP QF00A PA6.10
LNP* THERMOCOMP* QF00A is a compound based on Nylon 6/10 containing 50% Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180 |
|
Polyram PlusTek PA801 Nylon 6.6 Copolymer for Injection Molding, Impact Modified
Impact modified Nylon 6.6 copolymer for injection molding application.Information provided by Polyram.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 50%RH; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 70G30HSLR BK099 Nylon 66
(Unverified Data**)
30% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G30HSLR BK099 is a 30% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol..
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf..
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80x10x4; ISO 179/1eA |
|
Eurostar Staramide RF008U PA66/6, 40% Glass Filled, Injection Molded
Staramide RF008U is a 40% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 40V S4)Information provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180/1A |
|
Addiplast Addilene J 120 M10 Polypropylene Copolymer
Low fluidity for extrusion or injectionInformation provided by Addiplast.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO Test |
|
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Conditioned)
Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO Test |
|
BASF Ultramid® 8253 HS BK-102 PA6 (Dry)
Ultramid 8253 HS BK-102 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying leve..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ASTM D256 |
|
BLUESTAR LXS 314 G10 PPE-HIPS, 10% Glass Filled
Typical Applications: Water industrial partsInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature 23.0 °C
|
6.66
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180 |
|
BASF Ultramid® A3K Q603 PA66 (Conditioned)
Description: Ultramid A3K Q603 is a general purpose PA6/6.Information provided by BASF
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | Conditioned; ISO 180/1A |
|
Addiplast Addinyl PMD 20104 Nylon 66
High molding rateInformation provided by Addiplast.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180 |
|
Polyram RamOfin PPC104 Polypropylene Copolymer
Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram.
|
|||