Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180
PolyOne Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® MG34LG ABS
Automotive: Low gloss ABS for unpainted interior applications.
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® MG94U ABS
High flow, UV stabilized ABS molding grade
Izod Impact, Notched (ISO) 18.0 kJ/m²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ASTM D256
PTS PPE-LXS110 PPE-PS
Typical Applications: Electrical partsUL94 V-0 Flame RetardantInformation provided by PTS LLC.
Izod Impact, Notched (ISO) 18.0 - 18.0 kJ/m²

@Temperature -30.0 - -30.0 °C
8.57 - 8.57 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 18.0 kJ/m² Grade Count:1
Overview of materials for Polyphthalamide (PPA), High Impact
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180/1eA
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This ..
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4mm, Cut; ISO 180/1A
SABIC Innovative Plastics SABIC PPCOMPOUND 9710 PP
SABIC® PPcompound 9710 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st..
Izod Impact, Notched (ISO) >= 18.0 kJ/m²
>= 8.57 ft-lb/in²
ISO 180-1A
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned
Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
DIN 53453
Schwartz Technical Plastics LAMIGAMID® 710 High Density Polyethylene
Application: chain-guides, cutting plates, linersInformation provided by Schwartz Technical Plastics GmbH
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
DIN 53453
Schwartz Technical Plastics LAMINEX® 2140 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled
Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH
Izod Impact, Notched (ISO) 18.0 kJ/m²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® X5100 PC+PBT (Europe-Africa-Middle East)
XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I).
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR
LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON MV006S PP
LNP* VERTON* MV006S is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Structural.
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON MV006SU PP (Europe-Africa-Middle East)
LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL GTX GTX963 PPE+PA (Europe-Africa-Middle East)
NORYL GTX963 is an unfilled impact modified material with excellent heat properties and good processability.
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL IN120 PPE+HIPS (Europe-Africa-Middle East)
NORYL IN120 is an unfilled material with a Vicat B/120 of 125 °C according ISO 306. NORYL IN120 has been developed for the interior automotive
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East)
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
Izod Impact, Notched (ISO) 18.0 kJ/m²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Verton RV008ESV PA 66
40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180
Polyram Polytron P30N11 Polypropylene, 30% Long Fiber Glass
A chemically coupled 30% long fiber glass reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180
Tisan TISLAMID® 6 30% Glass Filled Impact Modified, Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym..
Izod Impact, Notched (ISO) 18.0 kJ/m²

@Temperature -40.0 °C
8.57 ft-lb/in²

@Temperature -40.0 °F
ISO Test
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry)
Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushion ..
Izod Impact, Notched (ISO) 18.0 kJ/m²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex..
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180/1A
Addiplast Addinyl B2 ZV40 Nylon 6, 40% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Izod Impact, Notched (ISO) 18.0 kJ/m²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
Polimeri Europa KOBLEND PCA 53 PC+ABS  (discontinued **)
Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ) and good light resistance. Vicat/B50 = 110°C Main application fiel..