| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 7.62e+17 ohm-cm | 7.62e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
|
|||
| Volume Resistivity | 7.62e+17 ohm-cm | 7.62e+17 ohm-cm | IEC 60093 |
|
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
|
|||
| Volume Resistivity | 7.62e+17 ohm-cm | 7.62e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
|
|||
| Volume Resistivity | 7.62e+17 ohm-cm | 7.62e+17 ohm-cm | IEC 60093 |
|
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
|
|||
| Volume Resistivity | 7.62e+17 ohm-cm | 7.62e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
|
|||
| Volume Resistivity | 7.62e+17 ohm-cm | 7.62e+17 ohm-cm | IEC 60093 |
|
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
|
|||