Physical Properties Metric English Comments
Melt Flow 5.6 g/10 min
5.6 g/10 min
ISO 1133:1997
Nanocyl PLASTICYL™ PP2001 Polypropylene with 2 wt% Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..
Melt Flow 5.6 g/10 min
<br>@Load 3.80 kg,<br> Temperature 230 °C
5.6 g/10 min
<br>@Load 8.38 lb,<br> Temperature 446 °F
ASTM D1238
SABIC Innovative Plastics Cycolac® MGABS02 ABS
General purpose ABS. Excellent flow/impact.
Melt Flow 5.6 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
5.6 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 4251R PPC+PC
High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors.
Melt Flow 5.6 g/10 min
<br>@Load 10.0 kg,<br> Temperature 230 °C
5.6 g/10 min
<br>@Load 22.0 lb,<br> Temperature 446 °F
ASTM D1238
Ineos ABS Centrex® 401 AES Extrusion &nbsp;(discontinued **)
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
Melt Flow 5.6 g/10 min
5.6 g/10 min
ASTM D1238
LyondellBasell Petrothene® NA217000 Low Density Polyethylene
ApplicationsPETROTHENE NA 217-000 is a high speed, lightweight coating resin for use with paper, films and other base stocks. This resin can yield coating weights down to 3.5 lbs/ream at line speed..
Melt Flow 5.6 g/10 min
5.6 g/10 min
ASTM D1238
LyondellBasell Petrothene® NA217080 Low Density Polyethylene
ApplicationsPETROTHENE NA 217-080 is a natural low density polyethylene resin formulated for use as primary insulation for coaxial and control cable applications. NA 217-080 has also been designed ..
Melt Flow 5.6 g/10 min
<br>@Load 10.0 kg,<br> Temperature 220 °C
5.6 g/10 min
<br>@Load 22.0 lb,<br> Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Melt Flow 5.6 g/10 min
<br>@Load 10.0 kg,<br> Temperature 220 °C
5.6 g/10 min
<br>@Load 22.0 lb,<br> Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Melt Flow 5.6 g/10 min
<br>@Load 5.00 kg,<br> Temperature 280 °C
5.6 g/10 min
<br>@Load 11.0 lb,<br> Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
Melt Flow 5.6 g/10 min
<br>@Load 5.00 kg,<br> Temperature 280 °C
5.6 g/10 min
<br>@Load 11.0 lb,<br> Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific)
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
Melt Flow 5.6 g/10 min
<br>@Load 5.00 kg,<br> Temperature 280 °C
5.6 g/10 min
<br>@Load 11.0 lb,<br> Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East)
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
Melt Flow 5.6 g/10 min
<br>@Load 5.00 kg,<br> Temperature 280 °C
5.6 g/10 min
<br>@Load 11.0 lb,<br> Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Melt Flow 5.6 g/10 min
<br>@Load 5.00 kg,<br> Temperature 280 °C
5.6 g/10 min
<br>@Load 11.0 lb,<br> Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Melt Flow 5.6 g/10 min
<br>@Load 5.00 kg,<br> Temperature 280 °C
5.6 g/10 min
<br>@Load 11.0 lb,<br> Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Melt Flow 5.6 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
5.6 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
Westlake EC4041AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC4041 is recommended for use in the boardstock coating industry. The resin has low neck-in and good drawdown characteristics. Coatings produced from EC4041 have ex..
Melt Flow 5.6 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
5.6 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238, ISO 1133
DuPont™ Fusabond® A560 Polymer Modifier
DuPont™ Fusabond® A560 is a chemically modified ethylene acrylate copolymer Used as a polymer modifier
Melt Flow 5.6 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
5.6 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
ASTM D1238
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene
Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer..
Melt Flow 5.6 g/10 min
<br>@Load 2.16 kg,<br> Temperature 235 °C
5.6 g/10 min
<br>@Load 4.76 lb,<br> Temperature 455 °F
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical..
Melt Flow 5.6 g/10 min
<br>@Load 2.16 kg,<br> Temperature 235 °C
5.6 g/10 min
<br>@Load 4.76 lb,<br> Temperature 455 °F
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical..
Melt Flow 5.6 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
5.6 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
Eastman D4041-P Polyethylene &nbsp;(discontinued **)
Low-density polyethylene D4041-P is a recommended for use in the boardstock coating industry for applications such as breadboard, cupstock, and liquid packaging board. This resin has low neck-in an..
Melt Flow 5.6 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
5.6 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
ASTM D1238
Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer &nbsp;(discontinued **)
Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold releaseApplications: Industrial covers and housings, Paper towel dispenser covers, Appliance partsInjection..