PolyOne Geon™ Vinyl Wire & Cable 3201-xx05D Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable 3201-xx05D Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
15 sec; ASTM D2240
Tensile Strength, Yield 12.4 MPa
1800 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 380 %
380 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
UL Temperature Rating
Brittleness Temperature -50.0 °C
-58.0 °F
ASTM D746
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
ALL; Internal Method
Processing Properties Metric English Comments
Melt Temperature 154 - 160 °C
309 - 320 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Agency Ratings UL QMFZ2
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Wire & Cable Applications