Polymer Property : Vicat Softening Point = 143 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® 144 PC
UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® 925 PC (Asia Pacific)
Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® 955AU PC (Asia Pacific)
Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® 9945A PC
Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® AD4820 PC (Europe-Africa-Middle East)
LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Lexan® FXD9945A PC (Asia Pacific)
UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® FXE163R PC (Europe-Africa-Middle East)
LEXAN FXE163R is a transparent/translucent UV stabilized, medium viscosity grade for special effects with fluorescent appearance. Color package may affect performance. LEXAN FXE163R contains a relea..
Vicat Softening Point 143 °C
289 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer
High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® HPS6 PC (Europe-Africa-Middle East)
Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. ..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® IR 2210 PC (Europe-Africa-Middle East)
PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele..
Vicat Softening Point 143 °C
289 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Lexan® LR180R PC (Europe-Africa-Middle East)
LR180R is a medium viscosity,release containing multipurpose polycarbonate industrial gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® VR2220 PC (Europe-Africa-Middle East)
VR2220 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® 925A PC
Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® 945U PC
Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® 955A PC
Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran..
Vicat Softening Point 143 - 157 °C
289 - 315 °F
Average value: 151 °C Grade Count:10
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
SABIC Innovative Plastics PC1000 PC (Europe-Africa-Middle East)
PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics PC1000R PC (Asia Pacific)
PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
SABIC Innovative Plastics PC1003R PC
PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was ..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics PC1003R PC (Asia Pacific)
PC1003R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF0335 PC (Europe-Africa-Middle East)
LNP* Lubricomp* LEXAN_LF0335 compound is a 35% glass fiber, milled glass reinforced PC injection moulding resin with improved wear resistance and reduced friction.
Vicat Softening Point 143 °C
289 °F
B/50; ISO R306
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact
High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries.
Vicat Softening Point 143 °C
289 °F
ASTM D1525
SK Chemicals SKYTHANE® S198A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific)
Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for..
Vicat Softening Point 143 °C
289 °F
50°C/h 50N; ISO 306
Covestro Makrolon® 2667 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection moldi..
Vicat Softening Point 143 °C
289 °F
50°C/h 50N; ISO 306
Covestro Makrolon® 6455 Polycarbonate, Flame Retardant Grade
MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmeasy releaseinjection moldingavailable in transparenttranslucent and opaque colorsPreprocessingMax. Water content
Vicat Softening Point 143 °C
289 °F
Covestro Makrolon® AL 2647 Polycarbonate, Automotive Lens Injection Grade
Easy flowing injection molding grade, UV-stabilized, easy mold release agent.Applications: Automotive lens applications, fulfills U.S. specification SAE J 576C.Information provided by Bayer.As of 1 ..
Vicat Softening Point 143 °C
289 °F
50°C/h 50N; ISO 306
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled
MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa..
Vicat Softening Point 143 °C
289 °F
B/50; ISO R306
Samsung Cheil Industries Infino® CF-1050 PC, Unreinforced High Impact
High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries.