Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 2.00 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179
PolyOne OnForce™ LFT AM-60LGF/001 Natural Polyphthalamide (PPA)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179
PolyOne OnForce™ LFT NN-50LGF/000 HS Black Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179
PolyOne OnForce™ LFT NN-50LGF/000 HS UV Black Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Charpy Impact, Notched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYabs X00 ABS, Extrusion Grade
Information provided by Polykemi AB
Charpy Impact, Notched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
Charpy Impact, Notched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 S20 Nylon 6 for injection molding
Nylon 6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer
FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C.
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eA
Pasargad Polymer Peyvand Pasamid 3P-H1000B Nylon 6
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® CLG902LX Acrylic Polymer
Information provided by Lucite International
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® C 216 V45 PA6, 45% glass fiber, Conditioned
Description: Polyamide PA6, reinforced with 45% of glass fiber, for injection molding.Available in: EuropeProduct Applications: TECHNYL C 216 V45 has been optimized to have high impact strength, a n..
Charpy Impact, Notched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East)
VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures.
Charpy Impact, Notched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
Charpy Impact, Notched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL GTX GTX964W PPE+PS+PA
Noryl GTX* GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications..
Charpy Impact, Notched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis RB607MO Polypropylene Random Copolymer
RB607MO is a random copolymer for blow molding, with good transparency and contact clarity, very good gloss and surface finish. Bottles up to 2 liters can be steam sterilized due to heat distortion ..
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® 1SVX-50H black 9288 PA1010-GF50
Product Description: Grilamid 1SVX-50H black 9288 is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile. Key properties of Grilamid 1SBVX-50H LDS ..
Charpy Impact, Notched 2.00 J/cm²

@Temperature 30.0 °C
9.52 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® AZ 3 PA66
Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures..
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® BG-30 S FA PA6-GF30
Product description: Grilon BG-30 S FA is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S FA has the following important properties: Excellent surface finishEasy ..
Charpy Impact, Notched 2.00 J/cm²

@Temperature 30.0 °C
9.52 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30
Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca..
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® TSG-35 PA666-GF35
Information provided by EMS Grivory
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® TSG-50/4 FA PA666-GF50
Information provided by EMS Grivory
Charpy Impact, Notched 2.00 J/cm²

@Temperature 30.0 °C
9.52 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® XE 4155 black 9992 PA612-I
Information provided by EMS Grivory
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope..
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® BG-50 PA6-GF50
Product description: Grilon BG-50 is a heat stabilized, normal viscosity PA6 injection molding grade with 50% glass fibers. Grilon BG-50 has the following important properties: High stiffnessGood su..
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
After conditioning at 23°C/50%RH; ISO 179/Af
Arkema Group Orgalloy® RS 6630 Polyamide 6.6 Alloy 30% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group
Charpy Impact, Notched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..
Copyright © lookpolymers.com All Rights Reserved