| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Europe-Africa-Middle East)
Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® 915R PC
Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties...
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® 915RP PC (Asia Pacific)
Lexan* 915RP Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® 916R PC (Europe-Africa-Middle East)
Lexan* 916R Polycarbonate (PC) resin is a low viscosity, non-filled, injection molding grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating at 0.8 mm properties. Lexan* ..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer
Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Europe-Africa-Middle East)
Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific)
ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system.
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® ML6413 PC (Asia Pacific)
Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® 945U PC (Europe-Africa-Middle East)
Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL WCA875 PPE-TPE
Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | Glow Wire Flammability Index, IEC 60695-2-12 |
|
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL LTA1350 PPE+PS
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL LTA5020 PPE+PS
Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS
Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 ..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS
Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng..
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East)
Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances.
|
|||
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East)
Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances.
|
|||
| Glow Wire Test | 800 °C | 1470 °F | Glow Wire Ignition Temperature; IEC 60695-2-13 |
|
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)
(Unverified Data**)