| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.26 g/cc | 1.26 g/cc | ASTM D792 |
| Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.150 % | 0.150 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.30 % | 0.30 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 8.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Melt Index of Compound | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 60.0 MPa | 8700 psi | 5 mm/min; ISO 527 |
| 62.0 MPa | 8990 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 72.0 MPa | 10400 psi | 5 mm/min; ISO 527 |
| 74.0 MPa | 10700 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 6.0 % | 6.0 % | Type I, 5 mm/min; ASTM D638 |
| 6.0 % | 6.0 % | 5 mm/min; ISO 527 | |
| Elongation at Yield | 3.0 % | 3.0 % | 5 mm/min; ISO 527 |
| 4.0 % | 4.0 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
| 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 | |
| Flexural Yield Strength | 114 MPa | 16500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 122 MPa | 17700 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 3.20 GPa | 464 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 3.50 GPa | 508 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
| 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Unnotched | 12.0 J/cm | 22.5 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*3; ISO 180/1A |
| 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB | NB | NB75; 80*10*3; ISO 180/1U |
| 73.0 kJ/m² @Temperature -30.0 °C |
34.7 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U | |
| Charpy Impact Unnotched | NB | NB | NB87; Edgew 80*10*3 sp=62mm; ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
NB85; Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
| Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 50.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 74.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 85.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 136 °C | 277 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 137 °C @Thickness 3.20 mm |
279 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ISO 306 |
| 149 °C | 300 °F | Rate B/120; ISO 306 | |
| 149 °C | 300 °F | Rate B/50; ASTM D1525 | |
| Flammability, UL94 | V-2 @Thickness 0.750 mm |
V-2 @Thickness 0.0295 in |
UL 94 by SABIC-IP |
| V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
UL 94 by SABIC-IP | |
| 5VB @Thickness 3.00 mm |
5VB @Thickness 0.118 in |
UL 94 by SABIC-IP | |
| 5VA @Thickness 3.00 mm |
5VA @Thickness 0.118 in |
UL 94 by SABIC-IP | |
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
| 875 °C | 1610 °F | IEC 60695-2-13 | |
| 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
| 175 - 250 V | 175 - 250 V | UL 746A | |
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
| High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | Pass | IEC 60695-10-2 |
| UV-light, water exposure/immersion | F1 | UL 746C |