Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Comparative Tracking Index = 250 V Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1...
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific)
Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Lexan® 4704 PPC (Asia Pacific)
High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Lexan® 955AU PC (Asia Pacific)
Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Lexan® FL920 PC
Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm).
Comparative Tracking Index 175 - 250 V
175 - 250 V
PLC code 3; UL 746A
SABIC Innovative Plastics Lexan® FXM141R PC
FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color ..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East)
Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstab..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Lexan® LUX9616 PC (Asia Pacific)
Lexan LUX9616 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme..
Comparative Tracking Index 175 - 250 V
<br>@Thickness 3.05 mm
175 - 250 V
<br>@Thickness 0.120 in
UL PLC 3 (175-250 V)
Resinoid 1340 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Comparative Tracking Index 175 - 250 V
<br>@Temperature 23.0 °C
175 - 250 V
<br>@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Rynite® FR515 BK507 PET &nbsp;(Unverified Data**)
Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific)
Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit..
Comparative Tracking Index 175 - 250 V
175 - 250 V
PLC 3
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Comparative Tracking Index 175 - 250 V
175 - 250 V
Average value: 213 V Grade Count:3
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Comparative Tracking Index 175 - 250 V
175 - 250 V
PLC code 3; UL 746A
SABIC Innovative Plastics Ultem 2412EPR PEI
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am..
Comparative Tracking Index 175 - 250 V
175 - 250 V
PLC code 3; UL 746A
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Valox® IQ4860HR PBT
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific)
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS
Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics NORYL PX1265 PPE+PS
Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL.
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized
Comparative Tracking Index 175 - 250 V
<br>@Thickness 0.750 mm
175 - 250 V
<br>@Thickness 0.0295 in
UL 746A
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT) &nbsp;(Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate  Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL PLC 3
Chang Chun Plastic Longlite PM T308J General Purpose Phenolic Molding Compound
ASTM Grade per ASTM D700 is 3.Information provided by Dowell Trading Company Ltd.
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer
Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based ..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific)
Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen..
Comparative Tracking Index 175 - 250 V
175 - 250 V
Average value: 219 V Grade Count:16
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Comparative Tracking Index 0.000 - 250 V
0.000 - 250 V
Average value: 138 V Grade Count:262
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
SABIC Innovative Plastics Lexan® HPH4504H PPC
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Copyright © lookpolymers.com All Rights Reserved