Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 GV20 Nylon 6 for injection molding, 20% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® 1600 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Charpy Impact, Notched | 1.00 - 1.36 J/cm² | 4.76 - 6.47 ft-lb/in² | Average value: 1.11 J/cm² Grade Count:4 |
Overview of materials for Chlorinated PVC (CPVC) This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179 eA |
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Europe-Africa-Middle East) NORYL SE90 is an unfilled, flame retardant material with a Vicat B/120 of 110°C according ISO 306. NORYL SE90 is V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, DRY Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics ULTEM 2300F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact compliant. Effective June, 2007 this grade will no longer be supported with .. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data, Low Temp |
Styron CALIBRE™ 5201 15 Polycarbonate, 20% Glass Reinforced CALIBRE® 5201 is a 20% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5201 resin exhibits high modulus and excellent dimensional stability.CALIBRE 52.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | double V-notch, rk=1.5 mm; DIN 53753 |
Zell-Metall Engineering Plastics Zellamid 1400T (PET + solid lubricant) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® TV4 640 (PBT+PC) - GF20 20% Glass Reinforced |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TSC-40/4 EC black 9832 PA666-CF40 Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 30.0 °C |
4.76 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30 PA666-GF30 Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® XE 4063 black 9238 PA6T/66-GF30 Product description: Grivory XE 4063 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 30.0 °C |
4.76 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4106 nat PA612-GF30 Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 30.0 °C |
4.76 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4106 nat PA612-GF30 Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Rynite® FR531 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Reinforced Flame Retardant Polyethylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® HT1V-45 HY black 9205 PA6T/6I-GF45 Product description: Grivory HT1V-45 HY black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-45 HY .. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BMF Nylon 11 (Conditioned) Designation ISO 1874-PA11,M,12-010Rigid grade for injection molding. Available color: natural. Additive free.Good melt viscosity. Outstanding ability to mold part with high length-thickness ratio an.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | |
Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, Dry as Molded
(discontinued **) Injection molding grade, higher stiffness, good stress corrosion cracking resistance and chemical resistance (fuel, cleaning agents).Information provided by Bayer.LANXESS was spun-off from Bayer in .. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Asia Pacific) Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region. |