| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glow Wire Test | 850 °C | 1560 °F | |
|
Plastcom SLOVASTER® B1 BT TS PBT, basic type
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
|
|||
| Glow Wire Test |
850
°C @Thickness 1.00 mm |
1560
°F @Thickness 0.0394 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® 1173X PC Copolymer (Europe-Africa-Middle East)
Lexan* 1173X polycarbonate (PC) resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-30 C) ductility in combination with high flow characteristics an..
|
|||
| Glow Wire Test |
850
°C @Thickness 1.00 mm |
1560
°F @Thickness 0.0394 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® 241RX PC (Europe-Africa-Middle East)
LEXAN 241RX is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.75 mm and allows for the molder to use up to 50 percent regri..
|
|||
| Glow Wire Test |
850
°C @Thickness 1.00 mm |
1560
°F @Thickness 0.0394 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® 244RF PC (Asia Pacific)
LEXAN 244RF resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors.
|
|||
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® 945AU PC
Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona..
|
|||
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® 9945A PC (Asia Pacific)
Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr..
|
|||
| Glow Wire Test |
850
°C @Thickness 1.60 mm |
1560
°F @Thickness 0.0630 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® AD143 PC (Asia Pacific)
LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission ..
|
|||
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER
Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. ..
|
|||
| Glow Wire Test |
850
°C @Thickness 0.800 mm |
1560
°F @Thickness 0.0315 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
|
|||
| Glow Wire Test |
850
°C @Thickness 1.00 mm |
1560
°F @Thickness 0.0394 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® FXD141R PC (Europe-Africa-Middle East)
LEXAN FXD141R is a transparent/translucent medium viscosity grade for light diffusion effects. Internal mold release. The color package may affect performance.
|
|||
| Glow Wire Test |
850
°C @Thickness 1.00 mm |
1560
°F @Thickness 0.0394 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® FXE101 PC (Europe-Africa-Middle East)
Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Glow Wire Test |
850
°C @Thickness 1.00 mm |
1560
°F @Thickness 0.0394 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® HP3AEU PC (Europe-Africa-Middle East)
Lexan HP3AEU resin is a medium flow polycarbonate with mold release designed for medical devices and pharmaceutical applications. It is assessed with biocompatible ISO10993 (or USP Class VI) and is..
|
|||
| Glow Wire Test |
850
°C @Thickness 1.00 mm |
1560
°F @Thickness 0.0394 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® HPS1 PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
|
|||
| Glow Wire Test |
850
°C @Thickness 1.00 mm |
1560
°F @Thickness 0.0394 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® HPS2 PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable..
|
|||
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® LUX2114 PC (Asia Pacific)
18 MFR. Improved flame retardance. Internal mold release. UV stabilized.
|
|||
| Glow Wire Test |
850
°C @Thickness 1.60 mm |
1560
°F @Thickness 0.0630 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® LUX2489D PC (Europe-Africa-Middle East)
Lexan LUX2489D is a polycarbonate resin with high reflective properties, UV additive, medium viscosity, injection molding grade exhibiting low dust attraction.
|
|||
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific)
Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop..
|
|||
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® LUX9612G PC (Europe-Africa-Middle East)
Lexan LUX9612G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p..
|
|||
| Glow Wire Test |
850
°C @Thickness 1.60 mm |
1560
°F @Thickness 0.0630 in |
IEC 60695-2-1 |
|
Polimeri Europa Edistir RK Polystyrene
(discontinued **)
UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl..
|
|||
| Glow Wire Test |
850
°C @Thickness 1.00 mm |
1560
°F @Thickness 0.0394 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® FXD164R PC (Europe-Africa-Middle East)
Transparent/translucent medium viscosity PC for light diffusion special effects, FDA compliant and mold release containing. The color package may affect performance.This data was supplied by SABIC-I..
|
|||
| Glow Wire Test |
850
°C @Thickness 2.00 mm, Time 5.00 sec |
1560
°F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
|
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin
Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar..
|
|||
| Glow Wire Test |
850
°C @Thickness 2.00 mm, Time 5.00 sec |
1560
°F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
|
LG Chemical Lupoy 1201HP-08 Polycarbonate Resin
Description: LUPOY PC 1201HP-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Glow Wire Test |
850
°C @Thickness 2.00 mm, Time 5.00 sec |
1560
°F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
|
LG Chemical Lupoy 1302-10 Polycarbonate Resin
Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Glow Wire Test |
850
°C @Thickness 2.00 mm, Time 5.00 sec |
1560
°F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
|
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin
Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Glow Wire Test |
850
°C @Thickness 3.00 mm |
1560
°F @Thickness 0.118 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
|
|||
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
|
|||
| Glow Wire Test |
850
°C @Thickness 2.00 mm |
1560
°F @Thickness 0.0787 in |
I.E.C. 695-2-1 |
|
Cossa Polimeri ESTACARB 1601 Polycarbonate
General purpose polycarbonateHigh melt flow rate, high impact resistanceInformation provided by Cossa Polimeri S.r.l.
|
|||
| Glow Wire Test | 850 °C | 1560 °F | < 30 sec; GB/2099.1 |
|
Zhejiang Juner PC-A1-2 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® HFD4412 PC
Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
|
|||
| Glow Wire Test |
850
°C @Thickness 3.00 mm |
1560
°F @Thickness 0.118 in |
IEC 60695-2-12 |
|
SABIC Innovative Plastics NORYL WCD835 PPE-TPE (Asia Pacific)