Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.20 GPa | 464 ksi | 1.5mm/min; ISO 178:2001 |
Nylacast Moly Cast Nylon 6, MoS2 Filled Nylacast Moly is part of the Cast Nylon 6 family. Its improved crystallization occurs by the addition of Molybdenum Disulphide. It includes MoS2, which is an extremely effective self dry lubricant w.. |
|||
Flexural Modulus | 3.20 GPa @Temperature 23.0 °C |
464 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH TS15040 D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP R1000S PA 66 LNP COLORCOMP* R1000S is an unfilled Nylon 66. Added features of this material is: Heat Stabilized. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178, ASTM D790 |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Flexural Modulus | 3.20 - 3.30 GPa @Temperature 60.0 - 120 °C |
464 - 479 ksi @Temperature 140 - 248 °F |
Average value: 3.27 GPa Grade Count:1 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | Tangent; ASTM D790 |
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2mm/min; ASTM D790 |
Kingfa PA66-ROW Halogen-free, Flame Retardant PA66 Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingConnectors, linkersRelay, bobbins, plugsHousehold appliance parts.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Lucite International Diakon® Frost 952 70 Acrylic Polymer Information provided by Lucite International |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Lucite International Diakon® Frost 952 80 Acrylic Polymer Information provided by Lucite International |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ASTM D790 |
Lucky IF-850 Acrylic, Injection Grade Easy-flow injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring .. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific) Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178-93 |
Wellman Wellamid® FR1841-N1 Nylon 66, Unfilled, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178-93 |
Wellman Wellamid® WE1359 25% Glass Sphere Filled, Toughened Nylon 66 Description: Glass Sphere Filled, Toughened Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2mm/min; ISO 178 |
Borealis MS64T20 Polypropylene Compound, Mineral Filled MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Lubrizol ESTALOC® 59300 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ASTM D 790 |
Cossa Polimeri ESTAPROP H 1080 T6 T D Polypropylene, 40% Mineral Filled PP homopolymer 40% mineral fillerGood physical and mechanical characteristics, high thermal stability, detergent resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | dry; ISO 178 |
DSM Stanyl® TS350 PA46 FR(17) Unreinforced, Flame Retardant |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 HWS Nylon 66, Finely Crystalline, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ASTM D790 |
Cast Nylons Nycast® 6PA-MoS2 Nylon 6 NYCAST® 6PA-MoS2 is a molybdenum disulphide filled Type 6 cast nylon. Finely divided MoS2 particles are suspended in the melt during polymerization. This gives the NYCAST® 6PA-MoS2 products improv.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ASTM D790 |
Chem Polymer Chemlon 102 Nylon 66, Nucleated A highly nucleated, lubricated nylon 66 intended for fast cycling applications. Increased tensile strength, rigidity, creep resistance and hardness over general purpose 66.Data provided by the manu.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | Dry; ISO 178 |
Arkema Group Orgalloy® RS 6010 Polyamide 6 Alloy 10% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ASTM D790 |
Ashley Polymers Ashlene® 291WO PPO A reinforced, flame retardant resin with outstanding structural strength. Good appearance and high impact.Data provided by the manufacturer |