Polymer Property : Specific Gravity = 1.26 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Stat-Tech™ PC-15CF/000 Black Polycarbonate (PC)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Nylene® Naxel™ PC45G FR 10% Glass Reinforced, Flame Retardant Polycarbonate
Description: Naxel™ PC45G FR is a 10% glass fiber reinforced, flame retardant polycarbonate. PC45G FR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins ar..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
S&E Specialty Polymers TufFill™ 5000-SN4 PP, Flame Retardant
Application: A No Bloom, UL 94 V-0 Polypropylene Compound TufFill™ 5000SN series is a specially engineered, low bloom, flame retardant polypropylene compound designed with halogen based technology...
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
SABIC Innovative Plastics Lexan® 505RU PC
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East)
Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Edgetek® PC-15CF/000 FCR Polycarbonate (PC)
The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Geon™ HTX M6215 Polyvinyl Chloride Alloy (PVC Alloy)
It is recommended that the compound pellets be dried for 3 to 4 hours at 150 deg. F.Information provided by PolyOne
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer
Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible A4D00 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible P484 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.26 g/cc
1.26 g/cc
Solvay Specialty Polymers Diofan® A602 Polyvinylidene Chloride (PVDC)  (discontinued **)
DIOFAN® A602 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features strong barrier prop..
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1-8379 Polyamide 66, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Specific Gravity 1.26 - 1.32 g/cc
1.26 - 1.32 g/cc
ASTM D 792
Karina E 36/145-GE Brown Color Concentrate for PVC
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.26 g/cc
1.26 g/cc
Momentive Performance Materials HV 3/806 Heat Cured Rubber - High Temperature
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D 792
SABIC Innovative Plastics Ultem HTX1010F PEI (Asia Pacific)
Higher impact, Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Teknor Apex APEX® 3800-90 Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor ..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing.
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
A. Schulman POLYBATCH™ Red 5400 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 5400 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5400 is heavy ..
Specific Gravity 1.26 g/cc
1.26 g/cc
Trelleborg R572 Natural Rubber Polyisoprene
All information provided by Trelleborg
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 2781
Lubrizol ESTANE® GP65DE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 65DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
A. Schulman POLYBATCH™ UVK-90 UV Stabilizer Concentrate Based In Polyethylene
DescriptionPOLYBATCH® UVK-90 is a UV stabilizer concentrate containing 10% hindered amine light stabilizer based in polyethylene. This concentrate is designed for use in LDPE, LLDPE, and HDPE appl..
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
A. Schulman POLYBATCH™ Red 5400 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 5400 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5400 is heavy ..
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 1183
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Specific Gravity 1.26 g/cc
1.26 g/cc
Method A; ASTM D792
LNP Thermocomp® SPS-F-1006 HS Syndiotactic Polystyrene, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..