Polymer Property : Charpy Impact, Notched = 1.00 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® C4220K PC+ABS (Asia Pacific)
Cycoloy* C4220K resin is an injection moldable 20% glass reinforced non FR PC-ABS. Key features include improved Knit Line strength, good flow, excellent strength & rigidity, heat resistance & hyd..
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS
High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics.
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER
LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an..
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific)
Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an..
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an..
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Europe-Africa-Middle East)
LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a..
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL B63 SG30 Nylon 6 for injection molding, 30% mineral filled
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179 eA
Lehmann & Voss LUVOCOM® 50/CF/10/GF/10/TF/10/BK Polycarbonate, with carbon fiber, glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Grupo Repol Dinalon® B1X25 G30V0 PA6 30% Glass Fiber, V0 Red Phosphorus and Halogen Free
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics ULTEM 2410EPR PEI
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific)
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics ULTEM PW2300 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified...
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East)
VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties.
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Europe-Africa-Middle East)
PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r..
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East)
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Europe-Africa-Middle East)
PC+Polyester, UV Stabilized, Transparent
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 353RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
DIN 53453
DSM Fibre Intermediates Nyrim® 2025 (Wollastocoat®), Conditioned
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Charpy Impact, Notched 1.00 J/cm²

@Temperature 30.0 °C
4.76 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50
Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® TSG-35/4 H black 9836 PA666-GF35
Product description: Grilon TSG-35/4 H is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® HT1V-45 HY black 9205 PA6T/6I-GF45
Product description: Grivory HT1V-45 HY black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-45 HY ..
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179
BASF Ultradur B 4406 G6 BKQ113 7110 30% Glass Filled PBT
Ultradur B 4406 G6 BKQ113 7110 is an UL V0 injection molding, pigmented black, PBT grade with 30% glass fiber reinforcement.
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eA
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® 304-G30 PBT Resin
30% glass fiber reinforced, flame retardant, low bleeding, UV-resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled
Injection molding, heat stabilizedInformation provided by PolyPlastic Group.
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Dry)
Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t..